Refine Your Search

Search Results

Viewing 1 to 3 of 3
Technical Paper

New Insights into the Unique Operation of Small Pore Cu-Zeolite SCR Catalyst: Overlapping NH3 Desorption and Oxidation Characteristics for Minimizing Undesired Products

2014-04-01
2014-01-1542
An operational challenge associated with SCR catalysts is the NH3 slip control, particularly for commercial small pore Cu-zeolite formulations as a consequence of their significant ammonia storage capacity. The desorption of NH3 during increasing temperature transients is one example of this challenge. Ammonia slipping from SCR catalyst typically passes through a platinum based ammonia oxidation catalyst (AMOx), leading to the formation of the undesired byproducts NOx and N2O. We have discovered a distinctive characteristic, an overlapping NH3 desorption and oxidation, in a state-of-the-art Cu-zeolite SCR catalyst that can minimize NH3 slip during temperature transients encountered in real-world operation of a vehicle.
Technical Paper

Development and Demonstration of a Soot Generator Integrated Bench Reactor

2014-04-01
2014-01-1589
Experimental evaluation of soot trapping and oxidation behaviors of various diesel particulate filters (DPF) has been traditionally hampered by several experimental difficulties, such as the deposition of soot particles with well-characterized and consistent properties, and the tracking of the soot oxidation rate in real time. In the present study, an integrated bench flow-reactor system with a soot generator has been developed and its capabilities were demonstrated with regards to: Consistently and controllably loading soot on DPF samples; Monitoring the exhaust gas composition by FTIR, including quantification of the soot oxidation rate using CO and CO2; Measuring soot oxidation characteristics of various DPF samples. Soot particles were produced from a laminar propane co-flow diffusion flame.
Technical Paper

Impact of Sulfur-Oxides on the Ammonia Slip Catalyst Performance

2014-04-01
2014-01-1545
The ammonia slip catalyst (ASC), typically composed of Pt oxidation catalyst overlaid with SCR catalyst, is employed for the mitigation of NH3 slip originating from SCR catalysts. Oxidation and SCR functionalities in an ASC can degrade through two key mechanisms i) irreversible degradation due to thermal aging and ii) reversible degradation caused by sulfur-oxides. The impact of thermal aging is well understood and it mainly degrades the SCR function of the ASC and increases the NH3 conversion to undesired products [1]. This paper describes the impact of sulfur-oxides on critical functions of ASC and on NH3 oxidation activity and selectivity towards N2, NOx and N2O. Furthermore impact of desulfation under selected conditions and its extent of ASC performance recovery is explained.
X