Refine Your Search

Search Results

Viewing 1 to 8 of 8
Technical Paper

A Comparison of the Mechanical Performance of AA6061-T6 Extrusions Subjected to Axial Crushing and Axial Cutting

2019-04-02
2019-01-1094
Conventional axially loaded energy absorbers dissipate kinetic energy through progressive folding. The significant fluctuations in load and high risk of transition to global bending are drawbacks that engineers have attempted to mitigate through several methods. A novel energy dissipation mechanism, referred to as axial cutting, utilizes thin-walled extrusions and a strengthened cutting tool to absorb energy in an axial impact. Compared to progressive folding, this can be achieved with minimal fluctuations in load during the deformation process. Based upon estimates from finite element models, a series of test cases were postulated where, for 8 and 10-bladed cutting scenarios, greater total energy absorption could be achieved through axial cutting than with progressive folding of geometrically similar extrusions. The specimens were AA6061 extrusions having T6 temper conditions that possessed 63.5 mm outer diameters and 1.5 mm wall thicknesses.
Journal Article

Experimental Investigation of Axial Cutting of AA6061 Extrusions under a Tension Deformation Mode

2020-04-14
2020-01-0206
A plethora of applications in the transportation industry for both vehicular and roadside safety hardware, especially seatbelts, harnesses and restraints, rely on tensile loading to dissipate energy and minimize injury. There are disadvantages to the current state-of-the-art for these tensile energy absorbers, including erratic force-displacement responses and low tensile force efficiencies (TFE). Axial cutting was extensively demonstrated by researchers at the University of Windsor to maintain a stable reaction force, although exclusively under compressive loading. A novel apparatus was investigated in this study which utilized axial cutting under a tensile loading condition to absorb energy. A parametric scope was chosen to include circular AA6061 extrusions in both T4 and T6 temper conditions with an outer diameter of 63.5 mm and wall thickness of 3.18 mm.
Technical Paper

Experimental Observations on the Mechanical Response of AZ31B Magnesium and AA6061-T6 Aluminum Extrusions Subjected to Compression and Cutting Modes of Deformation

2017-03-28
2017-01-0377
Cylindrical extrusions of magnesium AZ31B were subjected to quasi-static axial compression and cutting modes of deformation to study this alloy’s effectiveness as an energy absorber. For comparison, the tests were repeated using extrusions of AA6061-T6 aluminum of the same geometry. For the axial compression tests, three different end geometries were considered, namely (1) a flat cutoff, (2) a 45 degree chamfer, and (3) a square circumferential notch. AZ31B extrusions with the 45 degree chamfer produced the most repeatable and stable deformation of a progressive fracturing nature, referred to as sharding, with an average SEA of 40 kJ/kg and an average CFE of 45 %, which are nearly equal to the performance of the AA6061-T6. Both the AZ31B specimens with the flat cutoff and the circumferential notch conditions were more prone to tilt mid-test, and lead to an unstable helical fracture, which significantly reduced the SEA.
Technical Paper

Finite Element Modeling of the Axial Crushing of AA6061 T4 and T6 and AA6063 T5 Structural Square Tubes with Circular Discontinuities

2005-04-11
2005-01-0703
This research focused on the energy absorption capabilities of axially loaded structures fabricated from aluminum alloy extruded tubing with a square cross section. Quasi-static compressive testing was used to examine the effects of dual centrally-located circular hole discontinuities on the energy absorption characteristics of the extrusion test specimens. In addition to previously characterized progressive buckling and global bending modes, collapse modes involving cracking and splitting were observed in several experimental tests. For this reason, finite element models of each test specimen were developed using a material model incorporating damage mechanics. The suitability of using shell elements versus solid elements to model these relatively thick walled structures was investigated. A good correlation was observed between the results of the experimental quasi-static compressive tests and the results of the finite element simulations conducted using LS-DYNA.
Technical Paper

Maximized Energy Absorption and an Investigation on Practical Limitations for the Axial Cutting and Hybrid Cutting/Clamping Deformation Modes

2021-04-06
2021-01-0285
The axial cutting deformation mode is a novel alternative to progressive folding, the current state-of-the-art, where the cutting scheme exhibits more favorable mechanical performance. By splitting the extrusion into multiple evenly spaced and near-identical petals a highly consistent force response can be achieved. Maximizing the energy absorbing capacity of a sacrificial energy absorber is a fundamental design challenge in the field of crashworthiness. Generating hybrid deformation modes by simultaneously combining multiple deformation mechanisms into a single safety system is a promising technique to achieve high capacity energy dissipation. However, these systems tend to be susceptible to transitioning deformation modes (e.g. from progressive folding to global bending) since the sacrificial material is often loaded at or near its capacity.
Journal Article

Mechanical Performance of Circular AA6061-T6 Extrusions Under Axial Cutting Deformation

2011-04-12
2011-01-0022
Dynamic and quasi-static axial cutting of circular AA6061-T6 extrusions with variable instantaneous wall thickness in the axial direction was completed to investigate the capability of controlling the load/displacement responses of the extrusions. Circular specimens considered for this research had an original nominal wall thickness of 3.175 mm, an external diameter of 50.8 mm, and a tube length of 300 mm. Variations of the wall thickness were completed by material removal of the extrusions using a CNC machine. Specially designed cutters having a block height of 20 mm, a blade tip width of 1.0 mm and a blade shoulder width of 3.0 mm were employed to generate the axial cutting deformation mode. Either one or two cutters were selected to initiate a single or dual cutting deformation. A curved deflector with a profile radius of 50.8 mm was used to flare the cut petalled sidewalk and facilitate the cutting system.
Technical Paper

Observations of the Relative Performance of Magnesium and Aluminum Steering Wheel Skeletons with Identical Geometry

2000-03-06
2000-01-0784
Automotive steering wheels depend on a structural skeleton made of steel, aluminum, or magnesium to be the basis for the mechanical properties of the finished part. The mechanical properties of concern are the fatigue properties and the crash performance. The purpose of this study was to evaluate the crash and the fatigue performance of a steering wheel skeleton fabricated by high pressure die casting. Two materials were used to produce two groups of wheels with identical geometry. The production part was designed, optimized and fabricated with AM50A magnesium. The production magnesium component met all of the regulatory design and performance requirements. A small sample run was made in a proprietary aluminum - magnesium alloy. The fatigue and crash properties were evaluated empirically. In fatigue testing, the aluminum skeletons displayed a significant improvement, with respect to the magnesium skeletons, in the number of cycles to failure at the loads tested.
Journal Article

Simulation of the Axial Cutting Deformation of AA6061-T6 Round Tubes Utilizing Eulerian and Mesh Free Finite Element Formulations

2008-04-14
2008-01-1117
Experimental and numerical studies have been completed on the deformation behaviour of round AA6061-T6 aluminum extrusions during an axial cutting deformation mode employing both curved and straight deflectors to control the bending deformation of petalled side walls. Round extrusions of length 200 mm with a nominal wall thickness of 3.175 mm and an external diameter of 50.8 mm were considered. A heat treated 4140 steel alloy cutter and deflectors, both straight and curved, were designed and manufactured for the testing considered. The four blades of the cutter had an approximate average thickness of 1.00 mm which were designed to penetrate through the round AA6061-T6 extrusions. Experimental observations illustrated high crush force efficiencies of 0.82 for the extrusions which experienced the cutting deformation mode with the deflectors. Total energy absorption during the cutting process was approximately 5.48 kJ.
X