AMS5841F - Cobalt-Nickel Alloy, Corrosion and Heat-Resistant, Bars, 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb (Nb) - 2.9Ti - 0.20Al - 9.0Fe, Vacuum Induction Plus Vacuum Consumable Electrode Melted, Solution Heat Treated for Work Strengthening

Details
Document Number: AMS5841F
Revision Number: F
Title
Cobalt-Nickel Alloy, Corrosion and Heat-Resistant, Bars, 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb (Nb) - 2.9Ti - 0.20Al - 9.0Fe, Vacuum Induction Plus Vacuum Consumable Electrode Melted, Solution Heat Treated for Work Strengthening
Scope
This specification covers a high strength, corrosion and heat-resistant cobalt-nickel-chromium alloy in the form of bars.