SAE International
SAE Standards Works
SAE International
Contact Us | Help | Shopping Cart
SAE Login

AS7482B - Studs, Corrosion and Heat Resistant Steel, UNS S66286, Tensile Strength 130 ksi, 1800 °F Solution Heat Treated, Aged Before Roll Threading Procurement Specification

Details
Document Number: AS7482B
Revision Number: B
Title
Studs, Corrosion and Heat Resistant Steel, UNS S66286, Tensile Strength 130 ksi, 1800 °F Solution Heat Treated, Aged Before Roll Threading Procurement Specification
Scope
This specification covers studs made from a corrosion and heat resistant, age hardenable iron base alloy of the type identified under the Unified Numbering System as UNS S66286. The following specification designations and their properties are covered: AS7482 130 ksi minimum ultimate tensile strength at room temperature 70 ksi stress-rupture strength at 1200 °F; AS 7482-1 130 ksi minimum ultimate tensile strength at room temperature 78 ksi minimum ultimate shear strength at room temperature; AS7482-2 130 ksi minimum ultimate tensile strength at room temperature.
Recent Activity
Date Type