Heat Treatment Cast Nickel Alloy and Cobalt Alloy Parts AMS2773F

This specification specifies the engineering requirements for heat treatment, by part fabricators (users) or their vendors or subcontractors, of parts made of cast nickel or cobalt alloys and of fabricated assemblies in which cast nickel or cobalt alloys are the primary structural components. This specification is not intended to provide requirements for heat treating operations that are a responsibility of the casting supplier in meeting the requirements of the casting commodity specification.
AMS2773F
2022-04-22
Latest
Revised
AMS2773E
2013-02-11
Historical
Revised
AMS2773D
2012-10-08
Historical
Revised
AMS2773C
2011-09-13
Historical
Revised
AMS2773B
2008-08-28
Historical
Revised
AMS2773A
2005-03-03
Historical
Revised
AMS2773
1999-01-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 9% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Heat Treatment Nickel Alloy and Cobalt Alloy Parts

AMS2774G

View Details

STANDARD

Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Extrusions, Rings, and Stock for Forgings and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1950 °F (1066 °C) Solution Heat Treated, Precipitation Hardenable

AMS5664G

View Details

STANDARD

Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, and Rings 53Ni - 19Cr - 11Co - 9.8Mo - 3.2Ti - 1.6Al - 0.006B Vacuum Melted, Solution Heat Treated Precipitation Hardenable

AMS5712L

View Details

Get Involved

Want to participate in updating this standard?

X