Browse Standards AMS4372B
Current REVISED 2022-08-05

Aluminum Alloy, Plate 3.5Cu - 1.0Li - 0.40Mg - 0.35Mn - 0.45Ag - 0.12Zr (2050-T34) Solution Heat Treated and Stress Relieved AMS4372B

This specification covers an aluminum-lithium alloy in the form of plate 0.500 to 6.500 inches (12.70 to 165.00 mm) in nominal thickness (see 8.6).
AMS4372B
2022-08-05
Latest
Revised
AMS4372A
2019-05-23
Historical
Revised
AMS4372
2018-03-23
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 10% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Steel Tubing (Seamless) Round 0.55ni 0.5cr 0.2mo (0.27 - 0.33c) Heat Treated (125,000 Tensile Strength)

AMS6531

View Details

STANDARD

Selective (Brush) Nickel Plating Low-Stressed, Hard Deposit

AMS2439A

View Details

STANDARD

Titanium Alloy, Bars and Rods 3Al - 8V - 6Cr - 4Mo - 4Zr Consumable Electrode Melted Solution Heat Treated and Centerless Ground or Peeled and Polished

AMS4958F

View Details

Get Involved

Want to participate in updating this standard?

X