Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 47.5Ni - 22Cr - 1.5Co - 9.0Mo - 0.60W - 18.5Fe Solution Heat Treated AMS5754N

This specification covers a corrosion and heat-resistant nickel alloy in the form of bars, forgings, flash welded rings, and stock for forging, flash welded rings, or heading.
AMS5754N
2019-04-11
Latest
Revised
AMS5754M
2012-10-11
Historical
Reaffirmed
AMS5754L
2002-08-21
Historical
Revised
AMS5754K
1995-12-01
Historical
Revised
AMS5754J
1990-01-01
Historical
Revised
AMS5754H
1984-01-01
Historical
Revised
AMS5754G
1977-07-01
Historical
Revised
AMS5754F
1968-11-01
Historical
Revised
AMS5754E
1965-09-01
Historical
Revised
AMS5754D
1961-07-01
Historical
Revised
AMS5754C
1960-11-01
Historical
Revised
AMS5754B
1960-06-01
Historical
Revised
AMS5754A
1960-01-01
Historical
Revised
AMS5754
1954-05-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 9% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Cobalt Alloy, Corrosion and Heat-Resistant, Bars, Forging Stock, Forgings, and Rings 52Co - 20Cr - 10Ni - 15W

AMS5759N

View Details

STANDARD

Cobalt Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 40Co - 22Cr - 22Ni - 14.5W - 0.07La Solution Heat Treated

AMS5772F

View Details

STANDARD

Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.006B - 0.05Zr Consumable Electrode or Vacuum Induction Melted 1825 to 1900 °F Solution Heat Treated

AMS5706N

View Details

Get Involved

Want to participate in updating this standard?

X