1973-02-01

Permissible Defects in Hydraulic Tubing 730624

Test methods and data are summarized to assist in establishing limits for defects in aircraft hydraulic tubing. The defects evaluated are (1) cracks as detectable by ultrasonic inspection after tube fabrication, and (2) service damage such as chafing and denting observed on aircraft. Permissible defect limits are listed for 6061T6 aluminum return lines, 3000 psi hydraulic tubing of 21Cr-6Ni-9Mn as well as 304 1/8 hard CRES, and 3A1-2.5V cold worked titanium. The performance requirements are outlined to which the defect samples were tested.

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 17% off list price.
Login to see discount.
Special Offer: Download multiple Technical Papers each year? TechSelect is a cost-effective subscription option to select and download 12-100 full-text Technical Papers per year. Find more information here.
We also recommend:
TECHNICAL PAPER

Drilling Mixed Stack Materials for the BOEING 787

2010-01-1867

View Details

TECHNICAL PAPER

Drilling Mixed Stack Materials for the BOEING 787

2010-01-1867

View Details

TECHNICAL PAPER

Solid-State Spot Welding (Friction Spot Welding and Friction Stir Spot Welding) as a Bonding Technique to Replace the Process of Riveting within the Aircraft Industry?

2011-01-2499

View Details

X