This procurement specification covers solid rivets and hollow end rivets made from a corrosion and heat resistant steel of the type identified under the Unified Numbering System as UNS S66286 and of 80 ksi single shear strength at room temperature.
This standard specifies the characteristics of the MJ profile metric series of screw threads, altered from ISO 68 M Profile, to include a mandatory controlled radius of 0.18042P to 0.15011P at the root of the external thread and with the minor diameter of both external and internal threads increased to provide a basic thread height of 0.5625H in order to accommodate the external thread maximum root radius.
This specification covers an aluminum alloy in the form of extruded bars, rods, and profiles 0.250 to 2.000 inches (6.35 to 50.80 mm) in nominal thickness and up to 32 square inches (206 cm2), inclusive, in cross-sectional area (see 8.5).
This specification covers a corrosion- and heat-resistant steel in the form of work-strengthened bars and wire, 1-1/4 inches (31.8 mm) and under in nominal diameter or least distance between parallel sides.
This specification covers a corrosion- and heat-resistant steel in the form of bars, wire, forgings, mechanical tubing, flash-welded rings, and stock for forging or flash-welded rings.
This specification covers an aluminum alloy in the form of extruded bars, rods, wire, profiles, and tubing, flash-welded rings fabricated from extruded stock, and stock for flash-welded rings (see 8.6).
This procurement specification covers tubular-shaped, coiled spring pins made of a corrosion resistant nickel base alloy of the type identified under the Unified Numbering System as UNS N07718.
This specification covers an aluminum alloy in the form of extruded bars, rods, wire, shapes, and tubing 5.000 inches (127.00 mm) and under in nominal diameter or least thickness (wall thickness of tubing) (see 8.5).
The test method describes the procedure for determination of the total acid number (TAN) of new and degraded polyol ester and diester-based gas turbine lubricants by the potentiometric titration technique. The method was validated to cover an acidity range of 0.05 to 6.0 mg KOH g-1. The method may also be suitable for the determination of acidities outside of this range and for other classes of lubricants.