Refine Your Search

Search Results

Viewing 1 to 2 of 2
Technical Paper

Evaluation of Alternatives to Electrodeposited Cadmium for Threaded Fasteners Applications (III)

2009-11-10
2009-01-3228
Since 2005, Alcoa Fastening Systems (AFS) and Lockheed Martin have been partnering to identify a Cadmium (Cd) plating replacement for threaded fasteners. Previously reported Phase I, II and III studies resulted in alternative coatings that indicated promise as suitable plating materials. Phase IV and V studies continued the program by testing two different fasteners (NAS1580 and NAS4452) manufactured in AFS facilities. Testing included plating material characterization such as coating thickness, torque-tension relationships, locking and breakaway torque measurements, salt spray (fog) corrosion, stress corrosion, and push-in and interference properties. Additionally, mechanical properties of the plated fasteners were tested (tensile, double shear, durability, and fatigue). Candidates included two electroplated zinc-nickel coating systems (Zn-Ni and Zn-Ni2) and an electrodeposited aluminum coating (AI).
Technical Paper

Evaluation of Alternatives to Electrodeposited Cadmium for Threaded Fastener Applications (II)

2008-09-16
2008-01-2312
Cadmium electroplating is coming under increasing pressure due to both environmental and worker safety issues. Since 2005, Alcoa Fastening Systems (AFS) and Lockheed Martin have been conducting a collaborative research program to identify the most appropriate fastener coating materials for a Cadmium (Cd) plating replacement. Four candidate coatings were selected for the initial Phase I evaluation: electroless nickel (EN), electroless nickel composite (EN-PTFE), electrodeposited surface mineralization based zinc-nickel (Zn-Ni), and electroplated aluminum (Al). The Phase I testing results indicated that the Zn-Ni and Al coatings were the best of the four candidates for Cd replacement. However, it is hard to conduct direct comparisons with different coating thicknesses, surface treatments, and lubrication among various Cd alternatives. Thus, further evaluation with more careful control of these parameters would be necessary.
X