Steel, Corrosion-Resistant, Bars, Wire, Forgings, and Tubing 14.5Cr - 4.0Mo - 1.2V (1.10-1.20C) Premium Quality for Bearing Applications, Double Vacuum Melted

2019-09-24
WIP
AMS5749G
This specification covers a premium aircraft-quality, corrosion-resistant steel in the form of bars, wire, forgings, mechanical tubing, and forging stock.<p>These products have been used typically for parts requiring a through-hardening, corrosion-resistant steel, operating under heavy loads at high speeds, requiring resistance to wear and softening at elevated temperatures, and subject to very rigid inspection standards, but usage is not limited to such applications.
Standard

Steel, Corrosion-Resistant, Sheet and Strip 18Cr - 8Ni (SAE 30301) Cold Rolled, 3/4 Hard, 175 ksi (1207 MPa) Tensile Strength

2019-09-24
WIP
AMS5902D
This specification covers a corrosion-resistant steel in the form of sheet and strip. These products have been used typically in fabrication of aircraft structural components requiring moderate forming and bending, but usage is not limited to such applications. Mechanical properties specified herein are obtained by cold working (strain hardening) and not by heat treatment. Therefore, the cold-worked product should not be heated to a temperature which adversely affects the mechanical properties or corrosion resistance before, during, or after fabrication.
Standard

Steel, Corrosion-Resistant, Sheet and Strip 19Cr - 9.2Ni (SAE 30304) Cold Rolled, 3/4 Hard, 175 ksi (1207 MPa) Tensile Strength

2019-09-24
WIP
AMS5912C
This specification covers a corrosion-resistant steel in the form of sheet and strip. These products have been used typically for applications requiring moderate forming and bending, but usage is not limited to such applications. Mechanical properties specified herein are obtained by cold working (strain hardening), and not by heat treatment. Therefore, the cold-worked product should not be heated to a temperature which adversely affects the mechanical properties or corrosion-resistance before, during, or after fabrication.
Standard

Steel, Corrosion-Resistant, Sheet and Strip 19Cr - 9.2Ni (SAE 30304) Cold Rolled, 1/2 Hard, 150 ksi (1034 MPa) Tensile Strength

2019-09-24
WIP
AMS5911C
This specification covers a corrosion-resistant steel in the form of sheet and strip. These products have been used typically for applications requiring moderate forming and bending, but usage is not limited to such applications. Mechanical properties specified herein are obtained by cold working (strain hardening), and not by heat treatment. Therefore, the cold-worked product should not be heated to a temperature which adversely affects the mechanical properties or corrosion-resistance before, during, or after fabrication.
Standard

Steel, Corrosion-Resistant, Sheet and Strip 19Cr - 9.2Ni (SAE 30304) Cold Rolled, Full Hard, 185 ksi (1276 MPa) Tensile Strength

2019-09-24
WIP
AMS5913C
This specification covers a corrosion-resistant steel in the form of sheet and strip. These products have been used typically for applications requiring moderate drawing and forming, but usage is not limited to such applications. Mechanical properties specified herein are obtained by cold working (strain hardening) and not by heat treatment. Therefore, the cold-worked product should not be heated to a temperature which adversely affects the mechanical properties or corrosion-resistance before, during, or after fabrication.
Standard

Steel, Corrosion-Resistant, Bars and Forgings, 11.5Cr - 10Ni - 1.0Al - 0.5Ti - 1.0Cu - 1.0W, Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated, Precipitation Hardenable

2019-09-24
WIP
AMS5929A
This specification covers a corrosion-resistant steel in the form of bars, forgings, and forging stock. These products have been used typically for heat-treated parts requiring stress corrosion resistance, along with a combination of high strength and high toughness up to 800 °F (427 °C) with good ductility and strength in the transverse direction, but usage is not limited to such applications. Certain design, processing procedures, or environmental conditions may cause these products to become susceptible to stress-corrosion cracking; ARP1110 recommends practices to minimize such conditions.
Standard

Steel, Corrosion and Heat-Resistant, Bars and Forgings 15.5Cr - 4.5Ni - 2.9Mo - 0.10N Solution Heat Treated, Sub-Zero Cooled, Equalized, and Over-Tempered

2019-09-24
WIP
AMS5743K
This specification covers a corrosion and heat-resistant steel in the form of bars, forgings, and forging stock. These products have been used typically for parts requiring oxidation resistance and high strength up to 800 °F (427 °C) and where such parts may require welding during fabrication, but usage is not limited to such applications.
Standard

Steel, Corrosion and Heat-Resistant, Sheet, Strip and Plate, 18Cr - 13Ni - 2.5Mo (SAE 30316), Solution Heat Treated

2019-09-23
WIP
AMS5524M
This specification covers a corrosion and heat resistant steel in the form of sheet, strip, and plate. These products have been used typically for parts requiring both corrosion and heat resistance up to 1600 °F (871 °C), but usage is not limited to such applications. At elevated temperatures, strength of this steel is slightly higher than, and oxidation resistance is similar to that of 18-8 type steels.
Standard

Steel, Corrosion Resistant, Sheet and Strip, 18Cr - 8Ni (SAE 30301) Cold Rolled, 185 ksi (1276 MPa) Tensile Strength

2019-09-23
WIP
AMS5519P
This specification covers a corrosion-resistant steel in the form of sheet and strip. These products have been used typically for parts requiring moderate drawing or forming and high strength, but usage is not limited to such applications. Mechanical properties specified herein are obtained by cold working (strain hardening) and not by heat treatment. Therefore, the cold-worked product should not be heated to a temperature which adversely affects the mechanical properties or corrosion resistance before, during, or after fabrication.
Standard

Steel, Corrosion Resistant, Sheet and Strip 18Cr - 8Ni Cold Rolled, 150 Ksi (1034 MPa) Tensile Strength

2019-09-23
WIP
AMS5518N
This specification covers a corrosion-resistant steel in the form of sheet and strip. These products have been used typically for parts requiring strength and moderate forming or bending, but usage is not limited to such applications. Mechanical properties specified herein are obtained by cold working (strain hardening) and not by heat treatment. Therefore, the cold-worked product should not be heated to a temperature which adversely affects the mechanical properties or corrosion resistance before, during, or after fabrication.
Standard

Steel, Corrosion and Heat-Resistant, Sheet, Strip and Plate, 18Cr - 10.5Ni - 0.40Ti (SAE 30321) Solution Heat Treated

2019-09-23
WIP
AMS5510T
This specification covers a corrosion and heat-resistant steel in the form of sheet, strip, and plate. These products have been used typically for parts requiring both corrosion and heat resistance, especially when such parts require welding during fabrication and for parts requiring oxidation resistance up to 1500 °F (816 °C) but useful at that temperature only when stresses are low, but usage is not limited to such applications.
Standard

Steel, Corrosion and Heat-Resistant, Bars, Wire, Forgings, Tubing, and Rings 13Cr - 2.0Ni - 3.0W Annealed

2019-09-23
WIP
AMS5616N
This specification covers a corrosion and heat resistant steel in the form of bars, wire, forgings, mechanical tubing, flash welded rings, and stock for forging, flash welded rings, or heading. These products have been used typically for parts requiring oxidation resistance up to 1000 degrees F (538 degrees C), but usage is not limited to such applications. Strength at the higher temperature is superior to that of the standard 12Cr type steel.