Refine Your Search

Topic

Search Results

Standard

Steel, Corrosion-Resistant, Bars, Wire, Forgings, and Tubing 14.5Cr - 4.0Mo - 1.2V (1.10-1.20C) Premium Quality for Bearing Applications, Double Vacuum Melted

2019-09-24
WIP
AMS5749G
This specification covers a premium aircraft-quality, corrosion-resistant steel in the form of bars, wire, forgings, mechanical tubing, and forging stock.<p>These products have been used typically for parts requiring a through-hardening, corrosion-resistant steel, operating under heavy loads at high speeds, requiring resistance to wear and softening at elevated temperatures, and subject to very rigid inspection standards, but usage is not limited to such applications.
Standard

Steel, Corrosion-Resistant, Bars, Wire, Forgings, Extrusions, and Rings 5.0Mn - 22Cr - 12.5Ni - 2.2Mo - 0.20Cb - 0.30N - 0.20V Solution Heat Treated

2019-09-24
WIP
AMS5764F
This specification covers a corrosion-resistant steel in the form of bars, wire, forgings, extrusions, flash welded rings, and stock for forging, extruding, or flash welded rings.

These produces have been used typically for parts requiring excellent corrosion resistance and high strength from -423 degrees to +1100 degrees F (-253 degrees to +593 degrees C) and for welded parts without subsequent heat treatment, but usage is not limited to such applications.

Standard

Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 21Cr - 20Ni - 20Co - 3.0Mo - 2.5W - 1.0(Cb+Ta) - 0.15N - 32Fe Solution Heat Treated

2019-09-24
WIP
AMS5769G
This specification covers a corrosion and heat resistant alloy in the form of bars, forgings, flash welded rings, and stock for forging, flash welded rings, or heading.

These products have been used typically for parts, such as turbine rotors, shafts, blades, and bolts, requiring high strength up to 1350 degrees F (732 degrees C) and oxidation resistance up to 1800 degrees F (982 degrees C), but usage is not limited to such applications.

Standard

Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 74Ni - 7.0Cr - 16.5Mo, Solution Heat Treated

2019-09-24
WIP
AMS5771G
This specification covers a corrosion and heat-resistant nickel alloy in the form of bars, forgings, flash welded rings, and stock for forging or flash welded rings. These products have been used typically for parts, such as turbine air-sealing components, requiring moderate strength up to 1400 °F (760 °C) and oxidation resistance up to 1600 °F (871 °C), particularly where a low coefficient of expansion is desirable, but usage is not limited to such applications.
Standard

Alloy, Corrosion and Heat Resistant, Bars, Forgings, and Rings, 50Ni 20Cr 20Co 5.8Mo 2.2Ti 0.45Al Consumable Electrode or Vacuum Induction Melted 2100°F (1149°C) Solution Heat Treated

2019-09-24
WIP
AMS5886D
This specification covers a corrosion and heat resistant nickel alloy in the form of bars, forgings, flash welded rings, and stock for forging or flash welded rings. These products have been used typically for parts requiring high strength up to 1500 degrees F (816 degrees C) and oxidation resistance up to 2000 degrees F (1093 degrees C), particularly those parts which are formed or welded and then heat treated to develop required properties, but usage is not limited to such applications.
Standard

Steel, Corrosion-Resistant, Sheet and Strip 18Cr - 8Ni (SAE 30301) Cold Rolled, 3/4 Hard, 175 ksi (1207 MPa) Tensile Strength

2019-09-24
WIP
AMS5902D
This specification covers a corrosion-resistant steel in the form of sheet and strip. These products have been used typically in fabrication of aircraft structural components requiring moderate forming and bending, but usage is not limited to such applications. Mechanical properties specified herein are obtained by cold working (strain hardening) and not by heat treatment. Therefore, the cold-worked product should not be heated to a temperature which adversely affects the mechanical properties or corrosion resistance before, during, or after fabrication.
Standard

Steel, Corrosion-Resistant, Sheet and Strip 19Cr - 9.2Ni (SAE 30304) Cold Rolled, 3/4 Hard, 175 ksi (1207 MPa) Tensile Strength

2019-09-24
WIP
AMS5912C
This specification covers a corrosion-resistant steel in the form of sheet and strip. These products have been used typically for applications requiring moderate forming and bending, but usage is not limited to such applications. Mechanical properties specified herein are obtained by cold working (strain hardening), and not by heat treatment. Therefore, the cold-worked product should not be heated to a temperature which adversely affects the mechanical properties or corrosion-resistance before, during, or after fabrication.
Standard

Steel, Corrosion-Resistant, Sheet and Strip 19Cr - 9.2Ni (SAE 30304) Cold Rolled, 1/2 Hard, 150 ksi (1034 MPa) Tensile Strength

2019-09-24
WIP
AMS5911C
This specification covers a corrosion-resistant steel in the form of sheet and strip. These products have been used typically for applications requiring moderate forming and bending, but usage is not limited to such applications. Mechanical properties specified herein are obtained by cold working (strain hardening), and not by heat treatment. Therefore, the cold-worked product should not be heated to a temperature which adversely affects the mechanical properties or corrosion-resistance before, during, or after fabrication.
Standard

Steel, Corrosion-Resistant, Sheet and Strip 19Cr - 9.2Ni (SAE 30304) Cold Rolled, Full Hard, 185 ksi (1276 MPa) Tensile Strength

2019-09-24
WIP
AMS5913C
This specification covers a corrosion-resistant steel in the form of sheet and strip. These products have been used typically for applications requiring moderate drawing and forming, but usage is not limited to such applications. Mechanical properties specified herein are obtained by cold working (strain hardening) and not by heat treatment. Therefore, the cold-worked product should not be heated to a temperature which adversely affects the mechanical properties or corrosion-resistance before, during, or after fabrication.
Standard

Steel, Corrosion-Resistant, Bars and Forgings, 11.5Cr - 10Ni - 1.0Al - 0.5Ti - 1.0Cu - 1.0W, Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated, Precipitation Hardenable

2019-09-24
WIP
AMS5929A
This specification covers a corrosion-resistant steel in the form of bars, forgings, and forging stock. These products have been used typically for heat-treated parts requiring stress corrosion resistance, along with a combination of high strength and high toughness up to 800 °F (427 °C) with good ductility and strength in the transverse direction, but usage is not limited to such applications. Certain design, processing procedures, or environmental conditions may cause these products to become susceptible to stress-corrosion cracking; ARP1110 recommends practices to minimize such conditions.
Standard

Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 45.5Ni - 25.5Cr - 3.2Co - 3.2Mo - 3.2W - 18.5Fe Solution Heat Treated

2019-09-24
WIP
AMS5717J
This specification covers a corrosion and heat resistant nickel alloy in the form of bars, forgings, flash welded rings, and stock for forging or flash welded rings.

These products have been used typically for parts requiring heat and oxidation resistance up to 2150 degrees F (1177 degrees C), particularly where such parts may require welding during fabrication, but usage is not limited to such applications.

Standard

Steel, Corrosion and Heat-Resistant, Bars and Forgings 15.5Cr - 4.5Ni - 2.9Mo - 0.10N Solution Heat Treated, Sub-Zero Cooled, Equalized, and Over-Tempered

2019-09-24
WIP
AMS5743K
This specification covers a corrosion and heat-resistant steel in the form of bars, forgings, and forging stock. These products have been used typically for parts requiring oxidation resistance and high strength up to 800 °F (427 °C) and where such parts may require welding during fabrication, but usage is not limited to such applications.
Standard

Steel, Corrosion-Resistant, Bars, Wire, Forgings, Rings, and Extrusions 13Cr - 8.0Ni - 2.2Mo - 1.1Al Vacuum Induction Plus Consumable Electrode Melted Solution Heat Treated, Precipitation Hardenable

2019-09-24
WIP
AMS5629J
This specification covers a corrosion-resistant steel in the form of bars, wire, forgings, flash welded rings, and extrusions 12 inches (305 mm) and under in nominal diameter, thickness or for hexagons, least distance between parallel sides, and stock of any size for forging, flash welded rings, or extrusion (see 8.7).