Refine Your Search

Search Results

Viewing 1 to 12 of 12
Technical Paper

Development of Austempered Ductile Iron Timing Gears

1997-11-17
973253
Austempered ductile iron (ADI) is a material having excellent mechanical properties and damping capacity. However practical mass production of ADI gears has not been possible due to ADI's poor machinability and distortion during the austempering heat treatment. With a new process method of carrying out hobbing before austempering when the material is in its soft condition, then austempering it and lastly, conducting the shave finishing process, we have diminished the above defects and developed practical ADI gears. These new gears generate less noise than ordinary nitrocarburized steel gears and are superior in pitting resistance.
Technical Paper

Application to Body Parts of High-Strength Steel Sheet Containing Large Volume Fraction of Retained Austenite

1998-02-23
980954
Several different steel sheets were tested for energy absorption, using hat square columns and dynamic crash testing. Results indicate that steel sheets containing large volume fraction of retained austenite have relatively high energy absorption. The relationship between retained austenite and energy absorption was analyzed. These special steel sheets have already been successfully used for production body parts, such a front-side-member, without difficulties arising in volume production.
Technical Paper

Collapse of Thin-Walled Curved Beam with Closed-Hat Section - Part 2: Simulation by Plane Plastic Hinge Model

1990-02-01
900461
This paper describes a calculating method to predict the quasi-static collapsing behaviors of spot-welded closed-hat section curved beams under axial compression. The overall deformat ions and the local buckling modes of beams were calculated using a geometrical model. Force-displacement relations were predicted by a elastic-plastic structural analysis method using the ‘plastic hinge’ concept. Collapsing tests were made on beams which are differenting section size, rotation angle, and metal sheet thickness. Comparisons between the calculated and experimental results of deformed shapes of beams, the local buckling modes and the force displacement relations are discussed.
Technical Paper

Development of thermoplastic elastomeric vacuum hose for engine control

2000-06-12
2000-05-0150
Vulcanized rubber hoses are difficult to recycle and have a complicated manufacturing process. Recently, we have developed the vacuum hose for engine control out of thermoplastic elastomers. As a result of this development, scrap material from the manufacturing process can be recycled and, in addition, about a 30 percent weight reduction and a 20 percent cost reduction are achievable by virtue of the lower specific gravity and by the more simplified manufacturing process. In order to assess the feasibility of using thermoplastic elastomers for vacuum hoses, we developed a heat aging simulation test method. This was achieved by first investigating the actual vehicle environmental conditions of currently used vacuum hoses by retrieving and examining these hoses from used vehicles. We then extrapolated what the condition of such hoses would be after being subjected to heat aging for 200,000 km of service in an actual vehicle, and applied this calculation to our newly developed hoses.
Technical Paper

A New Oxygen Storage Componented Oxygen Sensor for the Emission Reductions of the Three-Way Catalyst System

1990-10-01
902120
A new prototype oxygen storage componented oxygen sensor has been developed which shows significant emission reductions of a 3-way catalyst system. This sensor is composed of ceria, as an oxygen storage component and supported pellets as a buffer layer surrounding the protective coating of the sensor element. This sensor offers a more rapid response than conventional ones under lean and rich fuel mixture excursions, which is caused by CO or O2 electrode poisoning.
Technical Paper

Development of a New Light-Weight Suspension Coil Spring

1993-03-01
930263
This newly developed helical spring can be used at a stress level up to 1300 MPa. The material is composed of Fe-C-Si-Mn-Ni-Cr-Mo-V alloy. Its strength-toughness balance was greatly superior to that of other spring steels. To improve the fatigue strength at a higher stress level, decarburization at the surface upon austenitizing was severely controlled, applying induction heating. Then, a special shot peening process, introduced for the first time, was applied to obtain a surface residual stress at the surface of over 1000 MPa. The spring was first applied to a 1992 TOYOTA model car. Plans are to increase the use since the spring material achieves a weight reduction of at least 30 % and, possibly, 35 to 40 %.
Technical Paper

Design and Testing of Ovate Wire Helical Springs

1993-10-01
932891
This paper describes the results of the study and research on ovate wire helical springs which have been jointly conducted by the members of the Japan Society for Spring Research consisting of the engineers from material suppliers, wire and spring producers and automotive manufacturers as well as researchers at Japanese universities. Attention is focused particularly on two types of wire cross sections, typical elliptical shape and Fuchs' egg-shape. Stresses on these two cross sections were analyzed by numerical calculations within the range of practical specification, and then the results have been compared with those of round wire spring. As a result, it has been found that the elliptical wire spring is superior to Fuchs- egg-shaped one for general application. Simple designing methods for the both types of wire helical springs have been developed based on the findings from the stress analysis.
Technical Paper

Reduction of Spiral Bevel Gear Noise in 4-Wheel Drive Vehicle Transfer System

1992-09-01
922109
Mitsubishi Motors Corporation uses spiral bevel gears in the transfer system for 4-wheel drive passenger cars modified from the front wheel drive configuration. This transfer gear ratio is near 1:1, and gears have uniform depth teeth cutting by the continuous generating method of OERLIKON cutting machine. In this method, the cutter and the work rotations are timed together to accomplish continuous indexing and cutting in order to enable high productivity. In general, it is difficult to reduce the meshing noise of spiral bevel gears and control its quality. The authors established the tooth surface coordinates, to reduce the meshing noise, by studying the influence of tooth surface coordinates on the meshing transmission error (MTE).
Technical Paper

Development of Hard Sintered Tappet and New Testing Method

1995-02-01
950389
We have developed a tappet with a cam lobe contacting tip made of a hard sintered material whose base material is cobalt, which adheres less to the steel of camshafts, and which also contains fine particles of tungsten carbide and chrome carbide. We have established a new evaluation method to access wear resistance performance of the tappet. It enables us to measure directly the friction force generated between the cam lobe and tappet and to evaluate anti-scuffing performance with high accuracy because we can clarify the time, load and cam angle at which scuffing occures.
Technical Paper

Numerical Analysis of Optimum Peening Condition in terms of Collision Energy on Coil Spring by Shot Peening

2005-04-11
2005-01-0798
This subject focuses on the simulated shot peening analysis of the collision energy and simulated collision energy distribution on coil spring. The authors studied hit condition by changing peening angle, and checked relationship between collision energy and residual stress. There have been no report that describe an analysis on the simulated shot peening effect on helical-shaped whereas reports on flat material exist1)2). In this paper, shot size, peening angle, spring wire overlapping are considered. The effectiveness of this analysis is verified in comparison with the previous test result where light was used to check the shadow of shot shower.
Technical Paper

Development of High-Strength Suspension Coil Springs in Which Corrosion Fatigue Strength is Important

2000-03-06
2000-01-0616
For the weight reduction of suspension coil springs for automobiles, high-strength steel has been developed. But, in general, strength and corrosion fatigue are contradictory. Then the technological basis is to raise durability and sag resistance, and further improvement of the corrosion fatigue strength is important. As a solution for the problem, element design which improved the performance against corrosion and optimum condition of shot peening process were studied. Thus high-strength suspension coil springs have superior corrosion fatigue strength, compared with the spring made of SAE9260 were developed. Moreover, as a new basic evaluation, corrosion fatigue test of springs with an artificial pit was worked out.
Technical Paper

Effects of Shot Peening and Grinding on Gear Strength

1994-03-01
940729
In recent year, higher strength for truck and bus transmission gear has become necessary. For the transmission gears, carburized gears have generally been used. We have examined the effects of shot peening and grinding using a CBN grindstone on the pitting strength and the bending fatigue strength of a carburized gear, and further evaluated a material which reduces the structual anomalies produced during carburization. As a result, it has been found that shot peening or CBN grinding is more effective for improving both pitting strength and bending fatigue strength than improving the material composition. Therefore, it is evident that residual compressive stress caused by shot peening or CBN grinding suppresses the propagation of cracks.