SURFACE TEXTURE CONTROL

1963-06-01
HISTORICAL
J449_196306
SAE J448, Surface Texture, has been set up for precision reference specimens using a controlled surface profile to obtain reproducible roughness values. These specimens are for instrument calibration. Appropriate symbols for roughness, waviness, and lay have also been standardized (ASA B46.1-1962 and SAE J448). For production control, especially from one geographical location to another, means are required to facilitate the inspection of surface characteristics called for by specifications which include not only roughness but profile waviness and lay. In order to integrate the requirements of the designer with the actual production of surfaces, a second grade of control standards must be adopted which will be functional in nature for the specific product being manufactured. These control standards may be Calibrated Pilot Specimens (actual parts with satisfactory texture) or Roughness Comparison Specimens (ASA B46.1-1962).
Standard

SURFACE TEXTURE CONTROL

1963-06-01
HISTORICAL
J449A_196306
SAE J448, Surface Texture, has been set up for precision reference specimens using a controlled surface profile to obtain reproducible roughness values. These specimens are for instrument calibration. Appropriate symbols for roughness, waviness, and lay have also been standardized (ASA B46.1-1962 and SAE J448). For production control, especially from one geographical location to another, means are required to facilitate the inspection of surface characteristics called for by specifications which include not only roughness but profile waviness and lay. In order to integrate the requirements of the designer with the actual production of surfaces, a second grade of control standards must be adopted which will be functional in nature for the specific product being manufactured. These control standards may be Calibrated Pilot Specimens (actual parts with satisfactory texture) or Roughness Comparison Specimens (ASA B46.1-1962).
Standard

Surface Texture Control

2011-08-04
CURRENT
J449_201108
SAE J448, Surface Texture, has been set up for precision reference specimens using a controlled surface profile to obtain reproducible roughness values. These specimens are for instrument calibration. Appropriate symbols for roughness, waviness, and lay have also been standardized (ASA B46.1-1962 and SAE J448). For production control, especially from one geographical location to another, means are required to facilitate the inspection of surface characteristics called for by specifications which include not only roughness but profile waviness and lay. In order to integrate the requirements of the designer with the actual production of surfaces, a second grade of control standards must be adopted which will be functional in nature for the specific product being manufactured. These control standards may be Calibrated Pilot Specimens (actual parts with satisfactory texture) or Roughness Comparison Specimens (ASA B46.1-1962).
Standard

Medical Device Shot Peening

2014-05-07
CURRENT
J3020_201405
This SAE Standard and its supplementary detail specifications cover the engineering requirements for the controlled shot peening of a medical device where shot peening is required for enhancement of a material's mechanical properties through the intentional creation of compressive residual stress.
Standard

SAE Manual on Blast Cleaning

2022-09-23
CURRENT
J792_202209
Blast cleaning may be defined as a mechanical pre-treatment process in which a suitable stream of solid particles is propelled with sufficient velocity against a work surface to cause a cleaning or abrading action when it comes in contact with the workpiece. Blast cleaning may be employed for a variety of purposes. It is a well-established method for removing sand from castings and burrs or scale from forgings, mill products, or heat treated parts; to promote machinability; and to minimize the possibility of interference in actual operation. In addition to this use, blast cleaning also produces a suitable surface for downstream industrial coatings. All these objectives are often accomplished in the one operation. As a general understanding, this document pertains to blast cleaning only. Any reference to shot peening or other processes is only to explain a context or concept related to blast cleaning.
Standard

SAE MANUAL ON BLAST CLEANING

1968-06-01
HISTORICAL
J792A_196806
Blast cleaning may be defined as a secondary manufacturing process in which a suitable stream of solid particles is propelled with sufficient velocity against a work surface to cause a cleaning or abrading action when it comes in contact with the workpiece. As indicated in the definition, blast cleaning may be employed for a variety of purposes. Ordinarily, it is considered as a method for removing sand from castings, burrs or scale from forgings, mill products, or heat treated parts; to promote machinability, and to minimize the possibility of interference in actual operation. In addition to this use, blast cleaning also produces an excellent surface for industrial coatings. All these objectives are often accomplished in the one operation.
Standard

Shot Peening

2015-06-30
CURRENT
J2441_201506
This SAE Standard covers the engineering requirements for peening surfaces of parts by impingement of metallic shot, glass beads, or ceramic shot.
Standard

Shot Peening

2000-08-01
HISTORICAL
J2441_200008
This SAE Standard covers the engineering requirements for peening surfaces of parts by impingement of metallic shot, glass beads, or ceramic shot.
Standard

CAST STEEL SHOT

1990-03-01
HISTORICAL
J827_199003
This SAE Recommended Practice describes chemical analysis, hardness, microstructure and physical characteristic requirements for cast steel shot to be used for shot peening or blast cleaning operations.
Standard

HIGH CARBON CAST STEEL SHOT

1994-07-01
HISTORICAL
J827_199407
This SAE Recommended Practice describes chemical composition, hardness, microstructure, and physical characteristic requirements for high carbon cast steel shot to be used for shot peening or blast cleaning operations.
Standard

HIGH-CARBON CAST-STEEL SHOT

1996-09-01
HISTORICAL
J827_199609
This SAE Recommended Practice describes chemical composition and physical characteristic requirements for high-carbon cast-steel shot to be used for shot peening or blast cleaning operations.
Standard

High-Carbon Cast-Steel Shot

2005-07-25
HISTORICAL
J827_200507
This SAE Recommended Practice describes chemical composition and physical characteristic requirements for high-carbon cast-steel shot to be used for shot peening or blast cleaning operations.
Standard

High-Carbon Cast-Steel Shot

2013-10-16
HISTORICAL
J827_201310
This SAE Recommended Practice describes chemical composition and physical characteristic requirements for high-carbon cast-steel shot to be used for shot peening or blast cleaning operations.
Standard

High-Carbon Cast-Steel Shot

2019-10-31
CURRENT
J827_201910
This SAE Recommended Practice describes chemical composition and physical characteristic requirements for high-carbon cast-steel shot to be used for shot peening or blast cleaning operations.
Standard

High-Carbon Cast-Steel Grit

2019-02-21
CURRENT
J1993_201902
This SAE Recommended Practice describes the chemical composition, and physical characteristic requirements for high-carbon cast-steel grit, to be used for blast cleaning and etching operations.
Standard

High-Carbon Cast-Steel Grit

2005-07-25
HISTORICAL
J1993_200507
This SAE Recommended Practice describes the chemical composition, and physical characteristic requirements for high-carbon cast-steel grit, to be used for blast cleaning and etching operations.
Standard

High-Carbon Cast-Steel Grit

2013-10-16
HISTORICAL
J1993_201310
This SAE Recommended Practice describes the chemical composition, and physical characteristic requirements for high-carbon cast-steel grit, to be used for blast cleaning and etching operations.