Journal Article

Off-Gassing and Particle Release by Heated Polymeric Materials

2008-06-29
2008-01-2090
Polymers are one of the major constituents in electrical components. A study investigating pre-combustion off-gassing and particle release by polymeric materials over a range of temperatures can provide an understanding of thermal degradation prior to failure which may result in a fire hazard. In this work, we report simultaneous measurements of pre-combustion vapor and particle release by heated polymeric materials. The polymer materials considered for the current study are silicone and Kapton. The polymer samples were heated over the range 20 to 400°C. Response to vapor releases were recorded using the JPL Electronic Nose (ENose) and Industrial Scientific's ITX gas monitor configured to detect hydrogen chloride (HCl), carbon monoxide (CO) and hydrogen cyanide (HCN). Particle release was monitored using a TSI P-TRAK particle counter.
Technical Paper

Monitoring Pre-Combustion Event Markers by Heating Electrical Wires

2009-07-12
2009-01-2543
Simultaneous measurements were made for particle releases and off-gassing products produced by heating electrical wires. The wire samples in these experiments were heated to selected temperatures in a heating chamber and responses to vapor releases were recorded by the JPL Electronic Nose (ENose) and an Industrial Scientific ITX gas-monitor; particles released were detected by a TSI P-Trak particle counter. The temperature range considered for the experiment is room temperature (24−26°C) to 500 °C. The results were analyzed by overlapping responses from the ENose, ITX gas sensors and P-Trak, to understand the events (particle release/off-gassing) and sequence of events as a function of temperature and to determine qualitatively whether ENose may be used to detect pre-combustion event markers.
X