Technical Paper

High Temperature Creep Behavior of Ceramic and Metal Substrates

1991-02-01
910374
The high temperature creep data for radial specimens, cut from metal and ceramic substrates and subjected to compressive loads representative of mounting and thermal pressure are presented as function of load and temperature. These data show that the creep resistance of metallic specimens under sustained loading varies with temperature and is orders of magnitude lower than that of ceramic specimens. The observed creep deformation in metallic specimens reduces their open frontal area and hydraulic diameter with potentially adverse impact on pressure drop across the metallic substrate.
Technical Paper

High Temperature Durability of Electrically Heated Extruded Metal Support

1994-03-01
940782
The design, performance and optimization of the extruded electrically heated metal converter have recently been published(1,2). The present paper focuses on the physical durability of extruded metal EHC support at high temperature representative of operating conditions. The mechanical, thermal, creep and fatigue properties of Fe-Cr-Al honeycomb structure over 25°-1000°C temperature range are reported. In addition, the stresses arising from mounting and thermal loads are computed via finite element analysis and compared with the high temperature strength of extruded metal EHC support. A safe design stress which predicts 192,000 kilometer durability is estimated from high temperature fatigue behavior of extruded Fe-Cr-Al honeycomb structure.
Technical Paper

High Temperature Compressive Strength of Extruded Cordierite Ceramic Substrates

1995-02-01
950787
High temperature modulus of rupture (MOR) data, published previously, show that the ceramic catalyst supports get stronger with temperature due to the absence of water vapor and closure of microcracks which would otherwise act as stress concentrators [1, 2 and 3]*. The increased MOR value is partially responsible for the excellent durability of ceramic catalyst supports at high temperature. In this paper, we will present the compressive strength data of ceramic substrates at high temperature, namely the crush strength along B-axis and biaxial compressive strength of the whole substrate. Since the honeycomb strength is directly related to that of the individual cell wall, the compressive strength should also increase with temperature similar to the modulus of rupture. Accordingly, the ceramic substrates are capable of supporting higher mounting pressures exerted by the intumescent mat at high temperature [4].