TUNGSTEN CARBIDE-COBALT COATING Detonation Process

1994-10-01
HISTORICAL
AMS2435E
This specification covers the engineering requirements for applying tungsten carbide/cobalt coatings to metal parts by the detonation process and the properties of such coatings.
Standard

Plating, Brush, Zinc-Nickel Low Hydrogen Embrittlement

2002-01-24
HISTORICAL
AMS2451/9
This specification covers the engineering requirements and process for brush plating of zinc-nickel by electrodeposition. It is used, in conjunction with AMS 2451, for corrosion-protective, zinc-nickel deposits, which may allow omission of hydrogen embrittlement relief treatment of high-strength steel.
Standard

Plating, Brush, Nickel Low Stress, Medium-Hardness Deposit

2000-08-01
HISTORICAL
AMS2451/7
This specification covers the engineering requirements and process for brush plating of medium-hardness, low stress nickel by electrodeposition. It should be used, in conjunction with AMS 2451, for medium-hardness, low stress nickel deposits.
Standard

Plating, Brush, Nickel Low Stress, Low-Hardness Deposit

1998-07-01
HISTORICAL
AMS2451/3
This specification covers the engineering requirements and process controls for selective plating of low-hardness, low-stress nickel by electrodeposition. It should be used, in conjunction with AMS 2451, for heat-resistant and corrosion-resistant nickel deposits.