Refine Your Search

Topic

Search Results

Technical Paper

Thin Wall Ceramic Catalyst Supports

1999-03-01
1999-01-0269
The stringent emissions regulations, notably for cold start, have led to design modifications in each of the converter components, notably the catalyst support. With the faster light–off requirement, the catalyst support must have a lower thermal mass so as to reach the 50% conversion temperature as quickly as possible. Simultaneously, for higher warmed–up efficiency, the catalyst support must offer higher geometric surface area. Similarly, for improved fuel economy and for preserving engine power, the catalyst support must exert lower back pressure. Indeed, these three performance requirements might be met by certain thin wall ceramic substrates, including 400/4.5 and 600/4.3, which have 22% lower thermal mass, 25% higher geometric surface area and 8% larger open frontal area than the standard 400/6.5 substrate. Testing by automakers and international laboratories on engine dynamometers has verified the above advantages of thin wall substrates.
Technical Paper

Thermal Stresses in Ceramic Wall Flow Diesel Filters

1983-02-01
830079
Thermal stresses constitute a major portion of the total stress which the ceramic wall flow filter experiences in service. The primary source of these stresses is the temperature gradients, both in radial and axial directions, which attain their maximum values during regeneration. The level of particulate loading, the flow rate, the filter size and the mounting design govern the severity of temperature gradients which, together with physical properties and aspect ratio of the filter, dictate the magnitude and distribution of thermal stresses. The filter, the mounting, and the regeneration conditions should be so designed as to minimize these stresses to insure reliable and fracture free performance of the filter throughout the lifetime of the vehicle. In this paper we present a thermal stress model, based on finite element method, which computes stresses in the axisymmetric filter subjected to linear or step temperature gradients in radial and axial directions.
Technical Paper

Thermal Shock Resistance of Oval Monolithic Heavy Duty Truck Converters

1988-02-01
880101
The long term durability of a heavy duty gasoline truck converter is addressed by examining thermal stresses due to radial temperature gradients under three different driving schedules. The pertinent physical properties of a catalyzed cordierite ceramic converter, with triangular cell structure, are first measured as function of temperature. These are followed by thermal mapping of mid-bed temperatures with the aid of thermocouples under various driving cycles on the truck dynamometer. Both the physical properties and the temperature distribution are then used as input parameters in the finite element thermal stress model to compute stresses in the oval converter.
Technical Paper

Thermal Durability of a Ceramic Wall-Flow Diesel Filter for Light Duty Vehicles

1992-02-01
920143
The thermal durability of a large frontal area cordierite ceramic wall-flow filter for light-duty diesel engine is examined under various regeneration conditions. The radial temperature distribution during burner regeneration, obtained by eight different thermocouples at six different axial sections of a 75″ diameter x 8″ long filter, is used together with physical properties of the filter to compute thermal stresses via finite element analysis. The stress-time history of the filter is then compared with the strength and fatigue characteristics of extruded cordierite ceramic monolith. The successful performance of the filter over as many as 1000 regenerations is attributed to three important design parameters, namely unique filter properties, controlled regeneration conditions, and optimum packaging design. The latter induces significant radial and axial compression in the filter thereby enhancing its strength and reducing the operating stresses.
Technical Paper

Systems Design for Ceramic LFA Substrates for Diesel/Natural Gas Flow- Through Catalysts

1995-02-01
950150
The monolithic, large frontal area (LFA), extruded ceramic substrates for diesel flow-through catalysts offer unique advantages of design versatility, longterm durability, ease of packaging and low Cost [1, 2]*. This paper examines the effect of cell density and cell size on catalyst light-off performance, back pressure, mechanical and thermal durability, and the steady-state catalytic activity. The factors which affect these performance characteristics are discussed. Certain trade-offs in performance parameters, which are necessary for optimum systems design, are also discussed. Following a brief discussion of design methodology, substrate selection, substrate/washcoat interaction and packaging specifications, the durability data for ceramic flow-through catalysts are summarized. A total of over 18 million vehicle miles have been successfully demonstrated by ceramic LFA catalysts using the systems design approach.
Technical Paper

Systems Approach to Packaging Design for Automotive Catalytic Converters

1990-02-01
900500
This paper addresses the packaging design for monolithic cordierite ceramic converters to meet the new, stringent durability requirements of the 1990's, while minimizing warranty cost for the automaker. These objectives are best met by using a systems approach during the early phases of packaging design, i.e. by examining design interactions between the ceramic monolith, alumina coating, ceramic mat or wiremesh mounting material with seals, stainless steel can, heatshields, and associated peripheral components. Failure of any one of these components can prove detrimental to converter durability. In this paper we take advantage of overall understanding of the observed failure modes and individual component behavior, and present new data for optimizing the total converter durability through initial design. In particular, the impact of symmetric gas entry, monolith contour, clamshell anisotropy, mount density, stiffener ribs, and heatshield insulation on total durability is highlighted.
Technical Paper

Substrate/Washcoat Interaction in Thin Wall Ceramic Substrates

1999-01-13
990013
Stringent emissions standards for HC, CO and NOx have necessitated the development of thin wall ceramic substrates which offer higher surface area, larger open frontal area and lower thermal mass. Such substrates offer the additional benefit of being compact which make them ideal for manifold mounting in the engine compartment. These attributes of ceramic substrates, following washcoat and catalyst application, translate directly into quick light-off, high conversion efficiency and low back pressure. To preserve these advantages at high operating temperature and still meet 100,000 mile vehicle durability, the thermomechanical interaction between the substrate and thin wall washcoat system must be managed carefully via formulation, % loading and the calcination process. This paper presents the physical properties data for thin wall ceramic substrates before and after the washcoat application.
Technical Paper

Strength and Thermal Shock Resistance of Segmented Wall-Flow Diesel Filters

1986-03-01
860008
The physical properties, including modulus of rupture, structural modulus and thermal expansion coefficient of segmented, large frontal area, ceramic wall-flow diesel filters are presented. The effect of cement composition, its coverage and segmentation pattern on these properties and on the failure modes during strength testing is discussed. Using these properties the mechanical and thermal integrities of LFA filter are computed and compared with those of monolithic filter,. The paper discusses both the high efficiency (EX-47, 100/17) and low efficiency (EX-66, 100/25) filter compositions.
Technical Paper

Size Effect on the Strength of Ceramic Catalyst Supports

1992-10-01
922333
The typical ceramic catalyst support for automotive application has a total volume of 1640 cm3. Approximately 10% of this volume is subjected to tensile thermal stresses due to a radial temperature gradient in service [1]*. These stresses are kept below 50% of the substrate strength to minimize fatigue degradation and to ensure long-term durability [2]. However, the tensile strength measurements are carried out in 4-point bending using 2.5 cm wide x 1.2 cm thick x 10 cm long modulus of rupture bars in which the specimen volume subjected to tensile stress is merely 3.2 cm3 or 0.2% of the total substrate volume [3]. Thus, a large specimen population is often necessary (50 specimens or more) to obtain the strength distribution representative of full substrate. This is particularly true for large frontal area substrates for diesel catalyst supports with an order of magnitude larger stressed volume. In this paper, the modulus of rupture data are obtained as function of specimen size.
Technical Paper

Robust Packaging System for Diesel/Natural Gas Oxidation Catalysts

1996-02-01
960471
The 290,000 vehicle-mile durability requirement for diesel/natural gas oxidation catalysts calls for robust packaging systems which ensure a positive mounting pressure on the ceramic flow-through converter under all operating conditions. New data for substrate/washcoat interaction, intumescent mat performance in dry and wet states, and high temperature strength and oxidation resistance of stainless steels, and canning techniques insensitive to tolerance stack-up are reviewed which help optimize packaging durability. Factors contributing to robustness of converter components are identified and methods to quantify their impact on design optimization are described. CERAMIC FLOW-THROUGH catalysts for diesel exhaust aftertreatment have met with much success since their introduction in 1993.
Technical Paper

Physical Durability of Thin Wall Ceramic Substrates

1998-10-19
982635
Significant advances in composition and the manufacturing process have led to thin wall cordierite ceramic substrates with low thermal mass, high surface area, and large open frontal area-properties that are critical for fast light-off, high conversion efficiency and low back pressure. Indeed, such substrates are ideal catalyst supports for meeting the ever-stringent emissions regulations, ala SULEV and ULEV, as demonstrated by recent performance data1. This paper focuses on the physical durability of 400/4 and 600/4 cordierite ceramic substrates. In particular, it presents strength, fatigue, and modulus data which influence the mechanical durability. In addition, it presents thermal expansion data which impact the thermal durability. Both of these durabilities are examined as a function of operating temperature.
Technical Paper

Performance and Durability of Advanced Ceramic Catalyst Supports

2003-01-18
2003-26-0015
As emissions regulations become more stringent, catalyst supports with higher cell density, smaller wall thickness, higher surface area and lower thermal mass become more desirable for faster light off and higher conversion efficiency. Simultaneously, however, washcoat formulation and loadings have to be adjusted to yield higher and more stable B.E.T. area at operating temperatures representative of close-coupled application. The thermal mass contribution of advanced washcoat system to catalyst supports with 600/4 and 900/2 cell structures may approach or even exceed that of uncoated substrates. Under such high washcoat loadings, the composite properties of advanced catalysts may be affected adversely in terms of their physical durability, notably in close-coupled application. This paper focuses on potential solutions to light-off performance and FTP efficiency, via optimization of substrate/washcoat interaction, geometric design and the mounting system.
Technical Paper

Performance Parameters for Advanced Ceramic Catalyst Supports

1999-10-25
1999-01-3631
The stringent emissions legislation has necessitated advances in the catalytic converter system comprising the substrate, washcoat technology, catalyst formulation and packaging design. These advances are focused on reducing light-off emissions at lower temperature or shorter time, increasing FTP efficiency, reducing back pressure and meeting the mechanical and thermal durability requirements over 100,000 vehicle miles. This paper reviews the role of cordierite ceramic substrate and how its design can help meet the stringent emissions legislation. In particular, it compares the effect of cell geometry and size on performance parameters like geometric surface area, open frontal area, hydraulic diameter, thermal mass, heat transfer factor, mechanical integrity factor and thermal integrity factor - all of which have a bearing on emissions, back pressure and durability. The properties of advanced cell configurations like hexagon are compared with those of standard square cell.
Technical Paper

Optimization of Substrate/Washcoat Interaction for Improved Catalyst Durability

1991-02-01
910372
The substrate/washcoat systems which preserve both the mechanical and thermal attributes of cordierite substrates are most desirable for prolonged durability of automotive catalysts. This paper provides a micromechanics viewpoint of substrate/washcoat composite whose properties are predictable, measurable and relevant to catalyst durability. The micromechanics model helps quantify substrate/washcoat interaction which controls the long-term catalyst performance. Three different examples of substrate/washcoat systems are used here to illustrate the optimization process during the development of new substrates or washcoat technologies to meet the more stringent emission and durability requirements of advanced catalysts for the 1990s.
Technical Paper

New Developments in Packaging of Ceramic Honeycomb Catalysts

1992-10-01
922252
The emissions regulations for the decade of 1990s are not only more stringent but are also required of vehicles other than passenger cars, for example both diesel and gasoline trucks as well as motorcycles. These latter applications involve different operating conditions in terms of space velocities, temperature profiles, and vibrational loads than those typical of passenger cars [1]*. In addition, the performance and durability requirements for these applications call for lower back pressure and longer service life. Furthermore, the space availability and the operating temperature range differ vastly so as to require special packaging designs to meet the durability requirements. This paper provides new data for ceramic insulating mats, both intumescent and non-intumescent [2,3], and ceramic substrates with thin and thick walls and square and triangular cell geometries [4], which are under development for non-passenger car applications indicated above.
Technical Paper

Mechanical Integrity of Ceramic Monolithic Converters

1981-11-01
811324
The converter assembly consists of a ceramic monolith with racetrack cross-section, a suitable “springy” mat wrapped around it and a clam-shell steel can to contain and guard these components against road hazards. The process to effect this assembly is rather dynamic and introduces directional loads onto the monolith in view of the anisotropic stiffness of the can. If these loads exceed certain values, they may cause failure of the monolith either by crushing it or by shearing it. In this paper we analyze the stiffness of various components of converter assembly, determine the load distribution around the monolith, and modify the design of can and monolith to make the load distribution more favorable. It is concluded that the converter assembly can be optimized and the failure of monoliths, if any, eliminated during closure. The present monoliths do not suffer from such failure.
Technical Paper

Measurement of Biaxial Compressive Strength of Cordierite Ceramic Honeycombs

1993-03-01
930165
The stringent durability requirements approaching 100,000 vehicle miles for automotive substrates and 290,000 vehicle miles for large frontal area diesel substrates for 1994+ model year vehicles call for advanced packaging designs with thick ceramic mats and high mount densities. The latter result in high mounting pressure on the substrate and enhance its mechanical integrity against engine vibrations, road shocks and back pressure forces. A novel measurement technique which applies a uniform biaxial compressive load on the lateral surface of ceramic substrates, thereby simulating canning loads, is described. The biaxial compressive strength data obtained in this manner help determine the maximum mounting pressure and mat density for a durable packaging design. The biaxial compressive strength data for both round and non round substrates with small and large frontal area are presented.
Technical Paper

Long-Term Durability of Ceramic Honeycombs for Automotive Emissions Control

1985-02-01
850130
Ceramic honeycomb structures have been used successfully as catalyst supports in gasoline-powered vehicles for the past ten years. They are currently the leading candidate for trapping and oxidizing the carbonaceous particulate emissions in diesel-powered vehicles. In both of these applications the long term durability of the ceramic substrate is of prime importance. This, in turn, depends on the physical properties of cellular structure, cyclic nature of service loads and design of the mounting assembly. This paper examines the nature and dependence of both the mechanical and thermal stresses in the substrate on its geometry, properties, mounting parameters, and the operating conditions. It also compares the observed failure modes with those predicted by the theory. The paper concludes with a set of recommendations for optimal systems design and acceptable operating conditions which will promote the long term durability of the ceramic substrate.
Technical Paper

Isostatic Strength of Porous Cordierite Ceramic Monoliths

1991-02-01
910375
The isostatic strength of porous cordierite ceramic monoliths plays an important role during canning and subsequent operation of automotive catalysts. Its value depends on wall porosity, cell geometry, skin thickness and morphology, monolith size and contour, and substrate/washcoat interaction. If the stresses induced by canning loads and closure speeds exceed the isostatic strength, the monolith may exhibit either crushing or shear type failure. This paper presents the room temperature isostatic strength data for coated and uncoated ceramic monoliths of different contour, size, and cell geometry. The applied isostatic load on the monolith is translated into stresses in the porous cell wall using both an analytical model and finite element analysis. It is found that the failure criteria are governed by the fundamental tensile and compressive strengths of the cell wall.
Technical Paper

Impact of Washcoat Formulation on Properties and Performance of Cordierite Ceramic Converters

1991-10-01
912370
The dual requirement of high conversion efficiency and 50K mile durability for cordierite ceramic converters is achievable through optimization of washcoat and catalyst formulation. This paper presents new data for high temperature physical properties, light-off performance, conversion efficiency and pressure drop through an oval cordierite ceramic converter with triangular cell structure and two different washcoat formulations; namely standard vs high-tech. Both of the washcoat systems have a beneficial effect on strength properties with nominal impact on thermal shock resistance. Both the standard and high-tech catalysts provide identical light-off performance for CO, HC and NOx conversion. The high-tech washcoat and catalyst system, in particular, provides consistently superior conversion efficiency for CO, HC and NOx. The pressure drop across the catalyst depends on hydraulic diameter and is only 8% higher for high-tech washcoat than for standard washcoat.
X