Journal Article

Effects on Surface Roughness and Friction on Aluminum Sheet under Plain Strain Cyclic Bending and Tension

2011-04-12
2011-01-0535
During sheet metal forming, the friction and surface roughness change as the sheet slides, bends and stretches against the tools. This study assessed evolution of friction and surface roughness changes on aluminum sheet with two surface finish conditions, mill finish (MF) and electron discharge texture (EDT), in both the longitudinal and the transverse rolling directions of the sheet. The sheets were tested using a three pin Draw Bead Simulator (DBS). Surface roughness of the sheet evolved as a result of bending at the first shoulder, reverse bending at the middle pin, bending at the second shoulder and unbending at the exit. Stretching conditions and sheet-pin contact were also varied to see the impact on surface roughness. In general, the largest surface roughness change for the transverse direction was observed at the convex side of the exit shoulder pin and on the convex side of the first shoulder for the longitudinal direction.
Journal Article

A Demonstration of Local Heat Treatment for the Preform Annealing Process

2011-04-12
2011-01-0538
The preform annealing process is a two-stage stamping method for shaping non age-hardenable (i.e. 5000 series) aluminum sheet panels in which the panel is heat treated in between the two steps to improve overall formability of the material. The intermediate annealing heat treatment eliminates the cold work accumulated in the material during the first draw. The process enables the ability to form more complex parts than a conventional aluminum stamping process. A demonstration of local annealing for this process was conducted to form a one-piece aluminum liftgate inner panel for a large sport utility vehicle using the steel product geometry without design concessions. In prior work, this process was demonstrated by placing the entire panel in a convection oven for several minutes to completely anneal the cold work.
X