Refine Your Search

Topic

Search Results

Standard

AIRCRAFT QUALITY STEEL CLEANLINESS Magnetic Particle Inspection Procedure

1978-07-01
HISTORICAL
AMS2301F
This specification covers steel cleanliness requirements for aircraft-quality ferromagnetic steels, other than hardenable corrosion-resistant steels, by magnetic particle inspection methods. Applicable primarily to blooms, billets, tube rounds, stock for forging or flash welded rings, slabs, bars, sheet, strip, plate, tubing, and extrusions used in fabricating parts subject to magnetic particle inspection, but may be used for qualification of a heat, melt, or lot of steel.
Standard

AIRCRAFT QUALITY STEEL CLEANLINESS Magnetic Particle Inspection Procedure

1974-12-01
HISTORICAL
AMS2301E
This specification covers steel cleanliness requirements for aircraft-quality ferromagnetic steels, other than hardenable corrosion-resistant steels, by magnetic particle inspection methods. Applicable primarily to blooms, billets, extrusions, tube rounds, heavy wall tubing, stock for forging and rings, tubing, bars, slab, and plate used in fabricating parts subject to magnetic particle inspection, but may be used for qualification of a heat, melt, or lot of steel.
Standard

AIRCRAFT QUALITY STEEL CLEANLINESS Magnetic Particle Inspection Procedure

1985-01-01
HISTORICAL
AMS2301G
This specification covers steel cleanliness requirements for aircraft-quality ferro-magnetic steels, other than hardenable corrosion-resistant steels, by magnetic particle inspection methods. Applicable primarily to blooms, billets, tube rounds, stock for forging or flash welded rings, slabs, bars, sheet, strip, plate, tubing, and extrusions used in fabricating parts subject to magnetic particle inspection, but may be used for qualification of a heat, melt, or lot of steel.
Standard

Chord Method of Evaluating Surface Microstructural Characteristics

2021-05-19
CURRENT
ARP1820C
This practice provides a method for evaluating microhardness and microstructure very close (0.002 inch (0.051 mm) or less) to the surface of a disk specimen. Specific accept/reject criteria for partial decarburization (3.7.1), inadvertent carburization/nitriding (3.7.3), total decarburization/intergranular oxidation (3.8), and other characteristics evaluated are to be found in the applicable specification where this ARP is referenced.
Standard

Control of Forgings Requiring First Article Approval

2017-07-10
HISTORICAL
AMS2375E
This specification covers procedures for obtaining first-article (preproduction) approval of forgings and the controls to be exercised in producing subsequent production forgings.
Standard

Control of Forgings Requiring First Article Approval

2022-09-23
CURRENT
AMS2375F
This specification covers procedures for obtaining first-article (preproduction) approval of forgings and the controls to be exercised in producing subsequent production forgings.
Standard

Gas Nitriding and Heat Treatment of Low-Alloy Steel Parts

2014-04-23
HISTORICAL
AMS2759/6B
This document specifies the procedure and requirements for heat treating low-alloy and tool steels and for their subsequent gas nitriding by the use of raw or dissociated ammonia. Specific process parameters are given for Nitralloy 135M, Nitralloy EZ, Nitralloy N, 4140, 4340, D6AC and H11 steels. Additional alloys and steel families (e.g., stainless steels) can also be nitrided using parameters acceptable to the cognizant engineering organization.
Standard

Gas Nitriding and Heat Treatment of Low-Alloy Steel Parts

2002-03-14
HISTORICAL
AMS2759/6A
This document specifies the procedure and requirements for heat treating low-alloy and tool steels and for their subsequent gas nitriding by the use of raw or dissociated ammonia. Specific process parameters are given for Nitralloy 135M, Nitralloy EZ, Nitralloy N, 4140, 4340, D6AC and H11 steels. Additional alloys and steel families (e.g., stainless steels) can also be nitrided using parameters acceptable to the cognizant engineering organization.
Standard

Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa)

2019-09-19
HISTORICAL
AMS2759/1H
This specification, in conjunction with the general requirements for steel heat treatment covered in AMS2759, establishes the requirements for heat treatment of carbon and low-alloy steel parts to minimum ultimate tensile strengths below 220 ksi (1517 MPa). Parts are defined in AMS2759. Due to limited hardenability in these materials, there are size limits in this specification.
Standard

Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa)

2018-04-28
HISTORICAL
AMS2759/1F
This specification, in conjunction with the general requirements for steel heat treatment covered in AMS2759, establishes the requirements for heat treatment of carbon and low-alloy steel parts to minimum ultimate tensile strengths below 220 ksi (1517 MPa). Parts are defined in AMS2759. Due to limited hardenability in these materials, there are size limits in this specification.