Subscribers can view annotate, and download all of SAE's content. Learn More »
Steel, Corrosion and Heat-Resistant, Bars and Wire 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V 1800 °F (982 °C) Solution Heat Treated and Work-Strengthened Consumable Electrode Remelted 200 ksi (1379 MPa) Tensile Strength Capability
AMS5726E
Steel Bars and Forgings, High Expansion 9.5No - 5.5Mn (0.55 - 0.65C) Annealed
AMS5623D
Steel, Corrosion Resistant, Bars and Wire 19Cr - 10Ni (304) High Yield Strength Solution Heat Treated and Cold Worked
AMS5857D
Want to participate in updating this standard?