Browse Standards AMS2280
Historical REAFFIRMED 2011-08-10

TRACE ELEMENT CONTROL Nickel Alloy Castings AMS2280

This specification establishes maximum permissible limits for elements not normally specified but which may occur in trace amounts in nickel alloy castings.
AMS2280D
2019-11-05
Latest
Revised
AMS2280C
2012-10-30
Historical
Revised
AMS2280
2011-08-10
Historical
Reaffirmed
AMS2280B
2006-09-22
Historical
Revised
AMS2280A
2000-09-01
Historical
Reaffirmed

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 9% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Castings, Alloy-Investment, 61ni 16cr 8.5co 1.8mo 2.6w 0.8cb 3.4ti 1.8ta 3.4al 0.010b 0.06zr (0.03-0.08c), Vacuum Melted, Vacuum Cast, as Cast

AMS5409A

View Details

STANDARD

Heat Treatment of Magnesium Alloy Castings

AMS2768C

View Details

STANDARD

Magnesium Alloy Castings, Sand 6.0Al - 3.0Zn (AZ63-T6) Solution and Precipitation Heat Treated

AMS4424L

View Details

Get Involved

Want to participate in updating this standard?

X