Browse Standards AMS2281B
Current STABILIZED 2013-01-17

Trace Element Control Nickel Alloy, Cobalt Alloy, and Iron Alloy Wrought Products for High-Temperature, High-Stressed Applications(STABILIZED Jan 2013) AMS2281B

This specification establishes maximum permissible limits for elements not normally specified but which may occur in trace amounts in wrought nickel, cobalt, and iron alloy products.