Rationale:
AMS2406N changes the hydrogen embrittlement relief requirement to the standard wording of 40 HRC for use with AMS2759/9, added hydrogen embrittlement relief requirement for hardnesses of 36-39 HRC and changes adhestion testing from an acceptance test to a periodic test.