ETCH INSPECTION OF HIGH STRENGTH STEEL PARTS AMS2649B

This specification establishes the requirements for etch inspection of bare high-strength low-alloy steel parts having tensile strength of 180 ksi (1241 MPa) and higher and of carburized parts to detect overheating caused by abusive machining or grinding in the heat treated condition. This process may remove 0.0001 to 0.0005 inch (2.5 to 12.7 μm) from the surface of the part.
AMS2649D
2019-07-15
Latest
Reaffirmed
AMS2649C
2008-01-03
Historical
Revised
AMS2649B
1996-10-01
Historical
Revised
AMS2649A
1996-06-01
Historical
Revised
AMS2649
1992-04-01
Historical
Reaffirmed

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 11% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Coating, Black Oxide

AMS2485L

View Details

STANDARD

Inspection of Ground, Chromium Plated Steel Parts

AMS2440C

View Details

STANDARD

Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa)

AMS2759/1H

View Details

Get Involved

Want to participate in updating this standard?

X