Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa) AMS2759/1F

This specification, in conjunction with the general requirements for steel heat treatment covered in AMS2759, establishes the requirements for heat treatment of carbon and low-alloy steel parts to minimum ultimate tensile strengths below 220 ksi (1517 MPa). Parts are defined in AMS2759. Due to limited hardenability in these materials, there are size limits in this specification.
AMS2759/1F
2018-04-28
Latest
Revised
AMS2759/1E
2014-04-23
Historical
Reaffirmed
AMS2759/1D
2007-06-13
Historical
Revised
AMS2759/1C
2000-09-01
Historical
Revised
AMS2759/1B
1996-12-01
Historical
Revised
AMS2759/1A
1996-09-01
Historical
Revised
AMS2759/1
1994-04-01
Historical
Revised

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 18% off list price.
Login to see discount.
Special Offer: Purchase more aerospace standards and aerospace material specifications and save! AeroPaks offer a customized subscription plan that lets you pay for just the documents that you need, when you need them.

Get Involved

Want to participate in updating this standard?

X