Browse Standards AMS4194D
Historical REAFFIRMED 2017-11-14

Aluminum Alloy, Sheet and Plate, Alclad 4.4Cu - 1.5Mg - 0.60Mn (2024 -T361 Sheet/Plate with 1½% Alclad) Solution Heat Treated, 6% Cold Worked and Naturally Aged(NONCURRENT Apr 1989) AMS4194D

This specification covers an aluminum alloy in the form of alclad sheet and plate supplied in the -T361 temper.
AMS4194E
2018-01-02
Latest
Revised
AMS4194D
2017-11-14
Historical
Reaffirmed
AMS4194C
2012-03-29
Historical
Reaffirmed
AMS4194B
1994-04-01
Historical
Revised
AMS4194A
1983-01-01
Historical
Revised
AMS4194
1970-11-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 10% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Aluminum Alloy, Sheet and Plate 6.3Cu - 0.30Mn - 0.18Zr - 0.10V - 0.06Ti (2219-O) Annealed or, When Specified, “As Fabricated” (2219-F)

AMS4031K

View Details

STANDARD

Aluminum Alloy, Sheet and Plate, Alclad 4.4Cu - 1.5Mg - 0.60Mn (2024-O with 1 ½% Alclad); Annealed

AMS4040P

View Details

STANDARD

Aluminum Alloy, Sheet and Plate, Alclad 4.4Cu - 1.5Mg - 0.60Mn (2024, -T3 Sheet/-T351 Plate with 1-1/2% Alclad) Solution Heat Treated, Cold Worked and Naturally Aged

AMS4041T

View Details

Get Involved

Want to participate in updating this standard?

X