Aluminum Alloy Castings 7.0Si - 0.35Mg (A356.0-T6) (Formerly T6P Temper) Solution and Precipitation Heat Treated AMS4218J

This specification covers an aluminum alloy in the form of sand, permanent mold, composite mold, and investment castings.
AMS4218J
2015-10-29
Latest
Reaffirmed
AMS4218H
2006-04-24
Historical
Reaffirmed
AMS4218G
1994-01-01
Historical
Revised
AMS4218F
1993-05-06
Historical
Revised
AMS4218E
1990-07-01
Historical
Revised
AMS4218D
1984-04-01
Historical
Revised
AMS4218C
1974-12-15
Historical
Revised
AMS4218B
1964-01-31
Historical
Revised
AMS4218A
1962-01-15
Historical
Revised
AMS4218
1961-01-15
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 10% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Aluminum Alloy, Investment Castings 7.0Si - 0.32Mg (356.0-T6) Solution and Precipitation Heat Treated

AMS4260G

View Details

STANDARD

Aluminum Alloy Castings 7.0Si - 0.55Mg - 0.12Ti - 0.06Be (A357.0 T6) Solution and Precipitation Heat Treated

AMS4219F

View Details

STANDARD

Aluminum Alloy, Castings 5.0Si - 1.2Cu - 0.50Mg (C355.0-T6) Solution and Precipitation Heat Treated

AMS4215J

View Details

Get Involved

Want to participate in updating this standard?

X