Historical ISSUED 2011-12-12

Aluminum Alloy, Sheet and Plate, Alclad 4.4Cu - 1.5Mg - 0.60Mn (Alclad 2024, -T361 Sheet & Plate) Solution Heat Treated, 6% Cold Worked and Naturally Aged AMS4466

This specification covers an aluminum alloy in the form of alclad sheet and plate supplied in the -T361 temper.
AMS4466B
2022-11-22
Latest
Revised
AMS4466A
2017-09-13
Historical
Revised
AMS4466
2011-12-12
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 10% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Aluminum Alloy, Sheet and Plate, Alclad 6.3Cu - 0.30Mn - 0.18Zr - 0.10V - 0.06Ti Alclad 2219-T81 Sheet Solution Heat Treated, Cold Worked, and Precipitation Heat Treated Alclad 2219-T851 Plate Solution Heat Treated, Stress Relieved, and Precipitation Heat Treated

AMS4094D

View Details

STANDARD

Aluminum Alloy, Sheet and Plate, Alclad 4.4Cu - 1.5Mg - 0.60Mn (Alclad 2024, -T3 Sheet, -T351 Plate) Solution Heat Treated, Cold Worked and Naturally Aged

AMS4462A

View Details

STANDARD

Aluminum Alloy, Coiled Sheet, Alclad 4.4Cu – 1.5Mg – 0.60Mn (Alclad 2024; -T4 Coiled Sheet) Solution Heat Treated

AMS4475B

View Details

Get Involved

Want to participate in updating this standard?

X