Browse Standards AMS4783F
Historical REAFFIRMED 2008-05-01

Cobalt Alloy, High Temperature Brazing Filler Metal 50Co - 8.0Si - 19Cr - 17Ni - 4.0W - 0.80B 2050 to 2100 °F (1121 to 1149 °C) Solidus-Liquidus Range AMS4783F

This specification covers a cobalt alloy in the form of wire, rod, strip, foil, and powder and a viscous mixture (paste) of the powder in a suitable binder.
AMS4783H
2021-07-07
Latest
Revised
AMS4783G
2014-12-11
Historical
Revised
AMS4783F
2008-05-01
Historical
Reaffirmed
AMS4783E
1995-12-01
Historical
Revised
AMS4783D
1992-04-01
Historical
Revised
AMS4783C
1991-07-01
Historical
Revised
AMS4783B
1985-07-01
Historical
Revised
AMS4783A
1978-07-15
Historical
Revised
AMS4783
1971-05-15
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 9% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Steel, Corrosion-Resistant, Bars, Wire, Forgings, and Tubing 16Cr - 2.5Ni (SAE 51431)

AMS5628F

View Details

STANDARD

Silver Alloy, Brazing Filler Metal 60Ag - 30Cu - 10Sn 1115 to 1325 °F (602 to 718 °C) Solidus-Liquidus Range

AMS4773H

View Details

STANDARD

Aluminum Alloy, Sheet and Plate, 0.12cu (1100-H14), Strain Hardened

AMS4003H

View Details

Get Involved

Want to participate in updating this standard?

X