Browse Standards AMS4916F
Historical Reaffirmed 1994-04-01

Titanium Alloy, Sheet, Strip, and Plate, 8al 1mo 1v, Duplex Annealed AMS4916F

This specification covers a titanium alloy in the form of sheet, strip, and plate. Primarily for parts requiring strength and fracture toughness up to 800 degrees F (427 degrees C). Certain processing procedures and service conditions may cause these products to become subject to stress-corrosion cracking; ARP982 recommends practices to minimize such conditions.
AMS4916L
2017-11-21
Latest
Revised
AMS4916K
2014-02-27
Historical
Reaffirmed
AMS4916J
2006-05-17
Historical
Revised
AMS4916H
2003-10-22
Historical
Revised
AMS4916G
2003-04-29
Historical
Revised
AMS4916F
1994-04-01
Historical
Reaffirmed
AMS4916E
1984-04-01
Historical
Revised
AMS4916D
1977-01-15
Historical
Revised
AMS4916C
1976-01-15
Historical
Revised
AMS4916B
1968-11-01
Historical
Revised
AMS4916A
1966-09-30
Historical
Revised
AMS4916
1966-03-15
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 18% off list price.
Login to see discount.
Special Offer: Purchase more aerospace standards and aerospace material specifications and save! AeroPaks off a customized subscription plan that lets you pay for just the documents that you neeed, when you need them.

Get Involved

Want to participate in updating this standard?

X