Titanium Bars, Wire, Forgings, and Rings Commercially Pure 70 ksi (483 MPa) Yield Strength AMS4921K

This specification covers one grade of commercially-pure titanium in the form of bars, wire, forgings, flash welded rings, and stock for forging or flash welded rings.
AMS4921R
2021-07-07
Latest
Revised
AMS4921P
2020-04-02
Historical
Revised
AMS4921N
2016-07-07
Historical
Revised
AMS4921M
2012-06-01
Historical
Revised
AMS4921L
2007-06-13
Historical
Revised
AMS4921K
2006-02-20
Historical
Revised
AMS4921J
2004-01-12
Historical
Revised
AMS4921H
2002-04-22
Historical
Revised
AMS4921G
1995-05-01
Historical
Reaffirmed
AMS4921F
1985-07-01
Historical
Revised
AMS4921E
1979-07-16
Historical
Revised
AMS4921D
1977-01-15
Historical
Revised
AMS4921C
1976-01-15
Historical
Revised
AMS4921B
1969-11-01
Historical
Revised
AMS4921A
1957-07-01
Historical
Revised
AMS4921
1952-11-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 10% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Hardness and Conductivity Inspection of Wrought Aluminum Alloy Parts

AMS2658D

View Details

STANDARD

Aluminum Alloy Forgings 7.7Zn - 2.5Mg - 1.5Cu - 0.16Cr (7049-01) High Temperature Annealed

AMS4321B

View Details

STANDARD

Aluminum Alloy Die Forgings 5.6Zn - 2.5Mg - 1.6Cu - 0.23Cr (7075-T73) Solution and Precipitation Heat Treated

AMS4141H

View Details

Get Involved

Want to participate in updating this standard?

X