Browse Standards AMS4928W
Current REVISED 2017-12-07

Titanium Alloy Bars, Wire, Forgings, Rings, and Drawn Shapes 6Al - 4V Annealed AMS4928W

This specification covers a titanium alloy in the form of bars, wire, forgings, flash welded rings, drawn shapes up through 10.000 inches (254.00 mm) inclusive in diameter or least distance between parallel sides and stock of any size for forging or flash welded rings.
AMS4928W
2017-12-07
Latest
Revised
AMS4928V
2016-06-15
Historical
Revised
AMS4928U
2014-03-07
Historical
Revised
AMS4928T
2013-08-15
Historical
Revised
AMS4928S
2011-06-23
Historical
Revised
AMS4928R
2007-01-09
Historical
Revised
AMS4928Q
2001-04-01
Historical
Revised
AMS4928P
2000-07-01
Historical
Revised
AMS4928N
1993-04-01
Historical
Revised
AMS4928M
1992-07-01
Historical
Revised
AMS4928L
1990-01-01
Historical
Revised
AMS4928K
1984-10-01
Historical
Revised
AMS4928J
1984-07-01
Historical
Revised
AMS4928H
1977-01-15
Historical
Revised
AMS4928G
1972-11-15
Historical
Revised
AMS4928F
1971-05-15
Historical
Revised
AMS4928E
1970-05-01
Historical
Revised
AMS4928D
1969-11-01
Historical
Revised
AMS4928C
1966-03-15
Historical
Revised
AMS4928B
1965-02-15
Historical
Revised
AMS4928A
1961-07-15
Historical
Revised
AMS4928
1957-07-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 11% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Steel, Corrosion-Resistant, Bars, Wire, Forgings, Mechanical Tubing, and Rings 16Cr - 4.0Ni - 0.30Cb (Nb) - 4.0Cu Solution Heat Treated, Precipitation Hardenable

AMS5643W

View Details

STANDARD

Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Rings, and Stock for Forgings and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 °F (968 °C) Solution Heat Treated, Precipitation-Hardenable

AMS5662P

View Details

STANDARD

Titanium Alloy, Bars, Wire, Forgings, and Rings 6.0Al - 4.0V Solution Heat Treated and Aged

AMS4965N

View Details

Get Involved

Want to participate in updating this standard?

X