Titanium Alloy Bars, Wire, and Forgings 7a1 4mo Solution and Precipitation Heat Treated AMS4970G

This specification covers a titanium alloy in the form of bars, wire, forgings, and forging stock.

This alloy has been used typically for parts requiring strength up to 900 degrees F (482 degrees C), but usage is not limited to such application.

Certain processing procedures and service conditions may cause these products to become subject to stress-corrosion cracking; SAE ARP 982 recommends practices to minimize such conditions.

AMS4970K
2016-09-20
Latest
Revised
AMS4970J
2012-09-25
Historical
Revised
AMS4970H
2008-02-15
Historical
Revised
AMS4970G
2003-03-14
Historical
Revised
AMS4970F
1994-04-01
Historical
Reaffirmed
AMS4970E
1994-04-01
Historical
Revised
AMS4970D
1978-07-15
Historical
Revised
AMS4970C
1970-05-01
Historical
Revised
AMS4970B
1969-11-01
Historical
Revised
AMS4970A
1966-03-15
Historical
Revised
AMS4970
1965-09-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 18% off list price.
Login to see discount.
Special Offer: Purchase more aerospace standards and aerospace material specifications and save! AeroPaks off a customized subscription plan that lets you pay for just the documents that you neeed, when you need them.

Get Involved

Want to participate in updating this standard?

X