Steel, Corrosion Resistant, Investment Castings 15Cr - 4.6Ni - 0.22Cb - 2.8Cu Solution and Precipitation Heat Treated (H1100) 130 ksi (896 MPa) Tensile Strength AMS5356D

This specification covers a corrosion resistant steel in the form of investment castings.
AMS5356D
2016-05-02
Latest
Revised
AMS5356
2011-08-10
Historical
Reaffirmed
AMS5356C
2010-02-24
Historical
Revised
AMS5356B
2006-04-18
Historical
Reaffirmed
AMS5356A
1995-05-01
Historical
Revised

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 10% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.

Due to current capacity constraints, printed versions of our publications - including standards, technical papers, EDGE Reports, scholarly journal articles, books, and paint chips - may experience shipping delays of up to four to six weeks. We apologize for any inconvenience.
We also recommend:
STANDARD

Steel, Corrosion-Resistant, Investment Castings 15Cr - 4.6Ni - 0.22Cb - 2.8Cu Solution and Precipitation Heat Treated (H935) 170 ksi (1172 MPa) Tensile Strength

AMS5400C

View Details

STANDARD

Steel, Corrosion-Resistant, Investment Castings 15Cr - 4.6Ni - 0.22Cb (Nb) - 2.8Cu Solution and Precipitation Heat Treated (H925) 180 ksi (1241 MPa) Tensile Strength (15-5)

AMS5346D

View Details

STANDARD

Steel, Investment Castings 0.95Cr - 0.20Mo (0.25 - 0.35C) (4130 Mod) Normalized or Normalized and Tempered

AMS5336J

View Details

Get Involved

Want to participate in updating this standard?

X