Browse Standards AMS5391
Historical ISSUED 1960-06-01

ALLOY CASTINGS, INVESTMENT, CORROSION AND HEAT RESISTANT Nickel Base - 13Cr - 4.5Mo - 0.75Ti - 6Al - 2.3(Cb+Ta) Vacuum Melted AMS5391

ALLOY CASTINGS, INVESTMENT, CORROSION AND HEAT RESISTANT Nickel Base - 13Cr - 4.5Mo - 0.75Ti - 6Al - 2.3(Cb+Ta) Vacuum Melted AMS5391 – available for purchase at $49.00. Find the right standards and certifications for your needs with SAE.
AMS5391H
2019-07-30
Latest
Reaffirmed
AMS5391G
2013-12-12
Historical
Revised
AMS5391C
2011-08-10
Historical
Reaffirmed
AMS5391F
2005-01-24
Historical
Revised
AMS5391E
1996-06-01
Historical
Revised
AMS5391D
1995-04-01
Historical
Revised
AMS5391B
1976-01-01
Historical
Revised
AMS5391A
1965-02-01
Historical
Revised
AMS5391
1960-06-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 10% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Alloy Castings, Sand, Corrosion and Heat Resistant 55Ni - 16.5Cr - 17Mo - 4.5W - 5.8Fe - 0.40V Solution Heat Treated

AMS5389D

View Details

STANDARD

Nickel Alloy, Corrosion and Heat-Resistant, Investment Castings 47.5Ni - 22Cr - 1.5Co - 9Mo - 0.60W - 18.5Fe (N-12MV) As-Cast

AMS5390G

View Details

STANDARD

Cobalt Alloy, Corrosion and Heat-Resistant, Investment Castings 54Co - 25.5Cr - 10.5Ni - 7.5W As-Cast

AMS5382K

View Details

Get Involved

Want to participate in updating this standard?

X