Browse Standards AMS5402D
Current REAFFIRMED 2023-05-16

Nickel Alloy, Corrosion- and Heat-Resistant, Investment Castings 62Ni - 21.5Cr - 9.0Mo - 3.6Cb (Nb) As Cast AMS5402D

This specification covers a corrosion and heat-resistant, air-melted, nickel alloy in the form of investment castings.
AMS5402D
2023-05-16
Latest
Reaffirmed
AMS5402C
2011-10-10
Historical
Reaffirmed
AMS5402A
2011-08-10
Historical
Reaffirmed
AMS5402B
1996-06-01
Historical
Revised
AMS5402
1980-01-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 10% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Nickel Alloy, Corrosion- and Heat-Resistant, Investment Castings 62Ni - 21.5Cr - 9.0Mo - 3.6Cb (Nb) Vacuum Melted, Vacuum Cast As Cast

AMS5401C

View Details

STANDARD

Steel Castings, Investment 0.80Cr - 1.8Ni - 0.35Mo (0.38 - 0.46C) (SAE 4340 Modified) Annealed

AMS5330E

View Details

STANDARD

Aluminum Alloy Castings, Investment 7.0Si - 0.32Mg (356.0-T51) Precipitation Heat Treated

AMS4261G

View Details

Get Involved

Want to participate in updating this standard?

X