Nickel Alloy, Corrosion and Heat Resistant, Seamless Tubing 52.5Ni 19Cr 3.0Mo 5.1Cb 0.90Ti 0.50Al 18Fe Consumable Electrode or Vacuum Induction Melted, 1775°F (968°C), Solution Heat Treated AMS5589B

This specification covers a corrosion and heat resistant nickel alloy in the form of seamless tubing.

This tubing has been used typically for fluid lines and components requiring resistance to creep and stress-rupture up to 1300 degrees F (704 degrees C) and oxidation resistance up to 1800 degrees F (982 degrees C), particularly those parts which are formed or welded and then heat treated to develop desired properties, but usage is not limited to such applications.

AMS5589F
2013-11-07
Latest
Revised
AMS5589B
2011-08-12
Historical
Reaffirmed
AMS5589E
2007-07-05
Historical
Revised
AMS5589D
2000-09-01
Historical
Revised
AMS5589C
1994-08-01
Historical
Revised
AMS5589A
1981-04-01
Historical
Revised
AMS5589
1966-09-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 18% off list price.
Login to see discount.
Special Offer: Purchase more aerospace standards and aerospace material specifications and save! AeroPaks offer a customized subscription plan that lets you pay for just the documents that you need, when you need them.

Get Involved

Want to participate in updating this standard?

X