Browse Standards AMS5590C
Historical Revised 1993-04-01

Nickel Alloy, Corrosion and Heat-Resistant, Seamless Tubing, 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe, Consumable Electrode or Vacuum Induction Melted 1950 °F (1066 °C) Solution Heat Treated AMS5590C

This specification covers a corrosion and heat resistant nickel alloy in the form of seamless tubing.

This tubing has been used typically for fluid lines and structural components requiring high strength at cryogenic temperatures and for short-time service up to 1200 degrees F (649 degrees C) and oxidation resistance up to 1800 degrees F (982 degrees C), particularly those parts which are formed or welded and then heat treated to develop desired properties, but usage is not limited to such applications.

AMS5590F
2010-06-16
Latest
Revised
AMS5590E
2006-04-19
Historical
Reaffirmed
AMS5590D
1995-04-01
Historical
Revised
AMS5590C
1993-04-01
Historical
Revised
AMS5590B
1991-10-01
Historical
Reaffirmed
AMS5590A
1981-04-01
Historical
Revised
AMS5590
1966-09-30
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 18% off list price.
Login to see discount.
Special Offer: Purchase more aerospace standards and aerospace material specifications and save! AeroPaks off a customized subscription plan that lets you pay for just the documents that you neeed, when you need them.

Get Involved

Want to participate in updating this standard?

X