Browse Standards AMS5596M
Current REVISED 2017-11-09

Nickel Alloy, Corrosion and Heat-Resistant, Sheet, Strip, Foil and Plate 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode Remelted or Vacuum Induction Melted 1775 °F (968 °C) Solution Heat Treated AMS5596M

This specification covers a corrosion and heat-resistant nickel alloy in the form of sheet, strip, foil, and plate 1.00 inch (25.4 mm) and under in thickness (see 8.5).
AMS5596M
2017-11-09
Latest
Revised
AMS5596L
2016-08-15
Historical
Revised
AMS5596K
2012-10-12
Historical
Reaffirmed
AMS5596J
1999-07-01
Historical
Revised
AMS5596H
1996-08-01
Historical
Revised
AMS5596G
1987-04-01
Historical
Revised
AMS5596F
1987-01-01
Historical
Revised
AMS5596E
1984-07-01
Historical
Revised
AMS5596D
1981-04-01
Historical
Revised
AMS5596C
1968-11-01
Historical
Revised
AMS5596B
1967-11-01
Historical
Revised
AMS5596A
1964-06-01
Historical
Revised
AMS5596
1964-01-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 10% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.

Due to current capacity constraints, printed versions of our publications - including standards, technical papers, EDGE Reports, scholarly journal articles, books, and paint chips - may experience shipping delays of up to four to six weeks. We apologize for any inconvenience.
We also recommend:
STANDARD

Nickel Alloy, Corrosion and Heat-Resistant, Sheet, Strip, and Plate 62Ni - 21.5Cr - 9.0Mo - 3.7 Cb (Nb) Annealed

AMS5599H

View Details

STANDARD

Steel, Corrosion Resistant, Sheet, Strip, and Plate 16.5Cr - 4.0Ni - 4.0Cu - 0.30Cb Solution Heat Treated, Precipitation Hardenable

AMS5604J

View Details

STANDARD

Steel, Corrosion and Heat-Resistant, Bars, Wire, Forgings, Tubing, and Rings 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V Consumable Electrode Melted 1800 °F (982 °C) Solution and Precipitation Heat Treated

AMS5732J

View Details

Get Involved

Want to participate in updating this standard?

X