Subscribers can view annotate, and download all of SAE's content. Learn More »
Steel, Corrosion-Resistant, Bars, Wire, and Forgings 12Cr - 8.5Ni - 1.2Ti - 2.0Cu Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated, Precipitation Hardenable
AMS5617K
Steel, Corrosion and Heat Resistant, Bars, Wire, and Forgings 12.5Cr - 0.75Ni - 1.0Mo - 1.0W - 0.24V (0.20-0.25C) Hardened and Tempered
AMS5655F
Steel, Corrosion and Moderate Heat Resistant, Bars, Forgings, and Rings, 14.5Cr - 6.5Ni - 0.72Ti, Solution Heat Treated and Maraged, 180,000 psi (1240 MPa) Tensile Strength
AMS5739E