Browse Standards AMS5637B
Historical REVISED 1971-05-01

Steel, Corrosion Resistant, Bars and Wire, 18Cr - 9.0Ni (SAE 30302), Solution Heat Treated and Cold Drawn, 125 ksi (862 MPa) Tensile Strength AMS5637B

This specification covers a corrosion-resistant steel in the form of bars and wire 0.75 inch (19 mm) and under in nominal diameter or distance between parallel sides.

These products have been used typically for small parts, such as bolts, screws, and clevis pins, requiring corrosion resistance up to 700 degrees F (371 degrees C) and which may be fabricated by heading or by machining from bars or wire and roll threading, but usage is not limited to such applications.

AMS5637J
2018-07-27
Latest
Revised
AMS5637H
2012-07-25
Historical
Revised
AMS5637E
2011-08-12
Historical
Reaffirmed
AMS5637G
2006-04-19
Historical
Reaffirmed
AMS5637F
2000-08-01
Historical
Reaffirmed
AMS5637D
1981-10-01
Historical
Revised
AMS5637C
1979-10-01
Historical
Revised
AMS5637B
1971-05-01
Historical
Revised
AMS5637A
1952-02-01
Historical
Revised
AMS5637
1949-03-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 18% off list price.
Login to see discount.
Special Offer: Purchase more aerospace standards and aerospace material specifications and save! AeroPaks offer a customized subscription plan that lets you pay for just the documents that you need, when you need them.

Get Involved

Want to participate in updating this standard?

X