Browse Standards AMS5637H
Historical REVISED 2012-07-25

Steel, Corrosion Resistant, Bars and Wire 18Cr - 9.0Ni (SAE 30302) Solution Heat Treated, Cold Drawn and Stress Relieved 125 ksi (862 MPa) Tensile Strength AMS5637H

This specification covers a corrosion resistant steel in the form of bars and wire 0.75 inch (19 mm) and under in nominal diameter or distance between parallel sides.
AMS5637K
2023-10-05
Latest
Revised
AMS5637J
2018-07-27
Historical
Revised
AMS5637H
2012-07-25
Historical
Revised
AMS5637E
2011-08-12
Historical
Reaffirmed
AMS5637G
2006-04-19
Historical
Reaffirmed
AMS5637F
2000-08-01
Historical
Reaffirmed
AMS5637D
1981-10-01
Historical
Revised
AMS5637C
1979-10-01
Historical
Revised
AMS5637B
1971-05-01
Historical
Revised
AMS5637A
1952-02-01
Historical
Revised
AMS5637
1949-03-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 11% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Steel, Corrosion Resistant, Bars and Wire 19Cr - 10Ni (304) High Yield Strength Solution Heat Treated and Cold Worked

AMS5857D

View Details

STANDARD

Steel, Corrosion-Resistant, Wire 19Cr - 9.5Ni (304) Solution Heat Treated

AMS5697G

View Details

STANDARD

Steel, Corrosion-Resistant, Sheet and Strip 18Cr - 9.0Ni (SAE 30302) Cold Rolled, Full Hard, 185 ksi (1276 MPa) Tensile Strength

AMS5906C

View Details

Get Involved

Want to participate in updating this standard?

X