Steel, Corrosion Resistant, Bars and Wire 18Cr - 9.0Ni (302) Solution Heat Treated, Cold Drawn and Stress Relieved 125 ksi (862 MPa) Tensile Strength AMS5637J

This specification covers a corrosion resistant steel in the form of bars and wire 0.75 inch (19 mm) and under in nominal diameter or distance between parallel sides (see 8.4).
AMS5637K
2023-10-05
Latest
Revised
AMS5637J
2018-07-27
Historical
Revised
AMS5637H
2012-07-25
Historical
Revised
AMS5637E
2011-08-12
Historical
Reaffirmed
AMS5637G
2006-04-19
Historical
Reaffirmed
AMS5637F
2000-08-01
Historical
Reaffirmed
AMS5637D
1981-10-01
Historical
Revised
AMS5637C
1979-10-01
Historical
Revised
AMS5637B
1971-05-01
Historical
Revised
AMS5637A
1952-02-01
Historical
Revised
AMS5637
1949-03-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 10% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Steel, Corrosion and Heat-Resistant, Bars and Wire 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V 1800 °F (982 °C) Solution Heat Treated and Work-Strengthened Consumable Electrode Remelted 200 ksi (1379 MPa) Tensile Strength Capability

AMS5726E

View Details

STANDARD

Steel, Corrosion and Heat-Resistant, Bars and Wire 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V Consumable Electrode Melted 1800 °F (982 °C) Solution Treated and Work-Strengthened Capable of 160 ksi (1103 MPa) Tensile Strength

AMS5853D

View Details

STANDARD

Steel, Corrosion-Resistant, Wire 19Cr - 9.5Ni (304) Solution Heat Treated

AMS5697G

View Details

Get Involved

Want to participate in updating this standard?

X