Steel, Corrosion Resistant, Bars, Wire, Forgings, Rings, and Extrusions 15Cr - 4.5Ni - 0.30Cb (Nb) - 3.5Cu Consumable Electrode Remelted Solution Heat Treated, Precipitation Hardenable AMS5659T

This specification covers a corrosion resistant steel in the form of bars, wire, forgings, flash welded rings, and extrusions in the solution heat treated condition (see 8.3), 12 inches (305 mm) and under in nominal diameter, thickness or for hexagons, least distance between parallel sides, and having a maximum cross-sectional area of 144 in2 (930 cm2), and stock of any size for forging, flash welded rings, or extruding.
AMS5659T
2021-10-01
Latest
Revised
AMS5659S
2016-08-15
Historical
Revised
AMS5659R
2015-04-10
Historical
Revised
AMS5659P
2014-02-27
Historical
Revised
AMS5659N
2012-09-24
Historical
Revised
AMS5659M
2008-12-17
Historical
Revised
AMS5659L
2004-01-14
Historical
Revised
AMS5659K
1998-11-01
Historical
Revised
AMS5659J
1995-03-01
Historical
Revised
AMS5659H
1995-03-01
Historical
Revised
AMS5659G
1990-01-01
Historical
Revised
AMS5659F
1984-10-01
Historical
Revised
AMS5659E
1984-07-01
Historical
Revised
AMS5659D
1984-01-01
Historical
Revised
AMS5659C
1976-07-01
Historical
Revised
AMS5659B
1966-09-01
Historical
Revised
AMS5659A
1966-03-01
Historical
Revised
AMS5659
1965-09-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 11% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Steel, Corrosion-Resistant, Bars, Wire, Forgings, Mechanical Tubing, and Rings 16Cr - 4.0Ni - 0.30Cb (Nb) - 4.0Cu Solution Heat Treated, Precipitation Hardenable

AMS5643W

View Details

STANDARD

Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Rings, and Stock for Forgings and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 °F (968 °C) Solution Heat Treated, Precipitation-Hardenable

AMS5662P

View Details

STANDARD

Steel, Corrosion Resistant, Bars, Wire, Shapes, and Forgings

AMSQQS763D

View Details

Get Involved

Want to participate in updating this standard?

X