Nickel-Iron Alloy, Corrosion and Heat-Resistant, Bars and Forgings 12.5Cr - 42.5Ni - 6.0Mo - 2.7Ti - 0.015B - 34Fe Consumable Electrode Remelted or Vacuum Induction Melted Solution, Stabilization, and Precipitation Heat Treated
AMS5660M
Cobalt-Nickel Alloy, Corrosion- and Heat-Resistant, Bars 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb (Nb) - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated and Work Strengthened
AMS5842H
Cobalt-Nickel Alloy, Corrosion- and Heat-Resistant, Bars 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb (Nb) - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated, Work Strengthened, and Aged
AMS5843H