Subscribers can view annotate, and download all of SAE's content. Learn More »
Nickel-Iron Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 42.5Ni - 12.5Cr - 5.8Mo - 2.9Ti - 0.015B - 35Fe Consumable Electrode or Vacuum Induction Melted Solution, Stabilization, and Precipitation Heat Treated
AMS5661G
Nickel Alloy, Corrosion and Heat Resistant, Sheet, Strip, and Plate 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1950 °F (1066 °C) Solution Heat Treated
AMS5597H
Rings, Flash Welded Corrosion and Heat-Resistant Austenitic Steels, Austenitic-Type Iron, Nickel or Cobalt Alloys, or Precipitation-Hardenable Alloys
AMS7490R