Nickel-Iron Alloy, Corrosion and Heat-Resistant, Bars and Forgings 12.5Cr - 42.5Ni - 6.0Mo - 2.7Ti - 0.015B - 34Fe Consumable Electrode Remelted or Vacuum Induction Melted Solution, Stabilization, and Precipitation Heat Treated
AMS5660M
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 72Ni - 15.5Cr - 0.95Cb(Nb) - 2.5Ti - 0.70Al - 7.0Fe 1800 °F (982 °C) Solution Heat Treated, Precipitation-Hardenable
AMS5670G
Steel, Corrosion-Resistant, Bars, Wire, Forgings, Mechanical Tubing, and Rings 15Cr - 6.5Ni - 0.75Mo - 0.30 Cb (Nb) - 1.5Cu Consumable Electrode Remelted, Solution Heat Treated Precipitation Hardenable