Browse Standards AMS5662L
Historical REVISED 2000-07-01

Nickel Alloy, Corrosion and Heat Resistant, Bars, Forgings, and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 °F (968 °C) Solution Heat Treated, Precipitation Hardenable AMS5662L

This specification covers a corrosion and heat resistant nickel alloy in the form of bars, forgings, flash welded rings, and stock for forging, flash welded rings, or heading.
AMS5662P
2022-08-17
Latest
Revised
AMS5662N
2016-06-21
Historical
Revised
AMS5662M
2009-06-11
Historical
Reaffirmed
AMS5662L
2000-07-01
Historical
Revised
AMS5662K
1998-01-01
Historical
Revised
AMS5662J
1994-09-01
Historical
Revised
AMS5662H
1994-08-01
Historical
Revised
AMS5662G
1993-01-01
Historical
Revised
AMS5662F
1989-01-01
Historical
Revised
AMS5662E
1985-10-01
Historical
Revised
AMS5662D
1979-07-01
Historical
Revised
AMS5662C
1972-05-01
Historical
Revised
AMS5662B
1967-11-01
Historical
Revised
AMS5662A
1966-03-15
Historical
Revised
AMS5662
1965-09-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 10% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Rings, and Stock for Forgings and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 °F (968 °C) Solution Heat Treated, Precipitation-Hardenable

AMS5662P

View Details

STANDARD

Nickel Alloy, Corrosion and Heat-Resistant, Bars, Wire, Forgings, and Rings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1975 °F (1079 °C) Solution Heat Treated

AMS5708M

View Details

STANDARD

Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 41.5Ni - 16Cr - 37Fe - 2.9Cb (Nb) - 1.8Ti Consumable Electrode Remelted or Vacuum Induction Melted 1750 °F (954 °C) Solution Heat Treated

AMS5702E

View Details

Get Involved

Want to participate in updating this standard?

X