AMS5663N: Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 °F (968 °C) Solution and Precipitation Heat Treated - SAE International
Browse Standards AMS5663N
Current REVISED 2016-06-20

Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 °F (968 °C) Solution and Precipitation Heat Treated AMS5663N

This specification covers a corrosion and heat-resistant nickel alloy in the form of bars, forgings, flash welded rings up to 10 inches (254 mm) in least cross-sectional dimension, having a maximum cross-sectional area of 78 in2 (503 cm2), and stock of any size for forging or flash welded rings (see 8.5).
AMS5663N
2016-06-20
Latest
Revised
AMS5663M
2009-06-11
Historical
Reaffirmed
AMS5663L
2003-07-14
Historical
Revised
AMS5663K
2002-11-21
Historical
Revised
AMS5663J
1997-09-01
Historical
Revised
AMS5663H
1996-01-01
Historical
Revised
AMS5663G
1989-07-01
Historical
Revised
AMS5663F
1989-01-01
Historical
Revised
AMS5663E
1987-04-01
Historical
Revised
AMS5663D
1980-10-01
Historical
Revised
AMS5663C
1972-05-01
Historical
Revised
AMS5663B
1967-11-01
Historical
Revised
AMS5663A
1966-03-01
Historical
Revised
AMS5663
1965-09-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 18% off list price.
Login to see discount.
Special Offer: Purchase more aerospace standards and aerospace material specifications and save! AeroPaks offer a customized subscription plan that lets you pay for just the documents that you need, when you need them.

Get Involved

Want to participate in updating this standard?

X